Mechanical Properties and Fractographic Analysis of High Manganese Steels After Dynamic Deformation Tests

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Stacking Fault Energy and Microstructural Insight into the Dynamic Deformation of High-Manganese TRIP and TWIP Steels

The dynamic behavior of three high manganese steels with very different stacking faultenergy (SFE) values (4-30 mJ/m2) were studied using high strain rate torsional tests. The hotrolledmicrostructure of the steel with the lowest SFE of 4 mJ/m2 consisted of a duplex mixture ofaustenite and ε-martensite, but those of the other two steels were fully austenitic. The deformedmicrostructures were stu...

متن کامل

Influence of High Strain Rates on the Mechanical Behavior of High-Manganese Steels

In this work, dynamic mechanical properties of three high-manganese steels with TRIP/TWIP or fully TWIP characteristics are studied. High strain rate experiments in the range of true strain rates between ~500 and 1800 /s are conducted using a dynamic torsional testing setup. All the three steels show a positive strain rate sensitivity in the intermediate range of strain rates (up to 500 /s). Bu...

متن کامل

determination of some physical and mechanical properties red bean

چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...

15 صفحه اول

The Effect of Deformation Temperature on the Mechanical Properties and Microstructural Evolutions of High Manganese TWIP Steel

In this study, the effect of tensile test temperature (148 to 673 K) on the microstructural evolutions and the mechanical properties of high manganese twinning induced plasticity (TWIP) steel with the chemical composition of Fe- 31Mn-3Al-3Si (wt. %) was investigated. XRD, SEM and TEM were used to study the microstructural evolutions. Stacking fault energy (SFE) of the alloy was also calculated ...

متن کامل

stacking fault energy and microstructural insight into the dynamic deformation of high-manganese trip and twip steels

the dynamic behavior of three high manganese steels with very different stacking faultenergy (sfe) values (4-30 mj/m2) were studied using high strain rate torsional tests. the hotrolledmicrostructure of the steel with the lowest sfe of 4 mj/m2 consisted of a duplex mixture ofaustenite and ε-martensite, but those of the other two steels were fully austenitic. the deformedmicrostructures were stu...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Archives of Metallurgy and Materials

سال: 2014

ISSN: 2300-1909

DOI: 10.2478/amm-2014-0207