Mechanical Stress Effects on 550 °C Hot Corrosion Propagation Rates in Precipitation Hardened Ni-Base Superalloys: CMSX-4, CM247LC DS and IN6203DS

نویسندگان

چکیده

Abstract Combinations of temperature, stress and hot corrosion may cause environmentally-assisted cracking in precipitation-hardened Ni-base superalloys, which is little understood. This research aims to increase current understanding by investigating the effects mechanical on propagation rate during corrosion-fatigue testing CMSX-4, CM247LC DS IN6203DS. The parameters used tests included a high R-ratio, frequency, temperature 550 °C. results showed CMSX-4 experienced predictable rate, also increased rates, but no obvious trend was apparent; whilst IN6203DS evidence an rate. These different behaviours appear be result interaction between microstructural features, include gamma-prime volume fractions both matrix eutectic regions, along with distribution structure. subsequently affected respective fatigue results, experiencing fracture significantly more scatter involved results. All specimens completed without cracking. It, therefore, appears that precipitation hardened are susceptible cracking, experience rates.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

Deformation Mechanisms in Ni-base Disk Superalloys at Higher Temperatures

This paper presents results from a research initiative aimed at investigating high temperature creep deformation mechanisms in Ni-base superalloys through a combination of creep experiments, TEM deformation mechanism characterization, and state of the art modeling techniques. The effect of microstructure on dictating creep rate controlling deformation mechanisms was revealed for specimens with ...

متن کامل

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...

متن کامل

Microstructural aspects of fatigue in Ni-base superalloys.

Nickel-base superalloys are primarily used as components in jet engines and land-based turbines. While compositionally complex, they are microstructurally simple, consisting of small (50-1000 nm diameter), ordered, coherent Ni(3)(Al,Ti)-type L1(2) or Ni(3)Nb-type DO(22) precipitates (called γ(') and γ(''), respectively) embedded in an FCC substitutional solid solution consisting primarily of Ni...

متن کامل

Microstructure and 3-d Effects in Fretting Fatigue of Ti Alloys and Ni-base Superalloys

Damage and plastic deformation accumulation in fretting fatigue occurs within a depth of a few crystallographic grains. Therefore, more accurate assumptions concerning length scale, damage volume, and the material model are needed to establish a more solid physical foundation necessary for next generation fretting fatigue damage prediction. Major thrusts include: (1) development and implementat...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Oxidation of Metals

سال: 2021

ISSN: ['0030-770X', '1573-4889']

DOI: https://doi.org/10.1007/s11085-021-10089-w