Mechanism of Initiation of Stress Corrosion Cracking in Smooth and Precracked Sheets of Austenitic Stainless Steels
نویسندگان
چکیده
منابع مشابه
Delayed Cracking of Metastable Austenitic Stainless Steels after Deep Drawing
In metastable austenitic stainless steels, strain-induced martensitic transformation during plastic deformation enhances work hardening of the material, increasing its strength and in some cases also ductility.1,2) The presence of α’-martensite, however, may increase the susceptibility of these materials to hydrogen embrittlement phenomena, for example delayed cracking.3–6) Delayed cracking can...
متن کاملAn Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution
The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...
متن کاملStress Corrosion Cracking of an Austenitic Stainless Steel in Nitrite-Containing Chloride Solutions
This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC) in a nitrite-containing chloride solution. Slow strain rate testing (SSRT) in 30 wt. % MgCl₂ solution established SCC susceptibility, as evidenced by post-SSRT fractography. Addition of nitrite to the chloride solution, which is reported to have inhibitive influence on corrosion of stainless ste...
متن کاملA Continuum Damage Model for the Stress Corrosion Cracking of Austenitic Stainless Steel
In the present work, the mechanical behavior of stress corrosion cracking phenomenon is described. Such phenomenon presents strong complexity due to metallurgic and electrochemical aspects. A methodology for modeling both SSR (Slow Strain Rate) and CL (Constant Load) tests based upon thermodynamics of continuum solids and elastoplastic damage is proposed. In this macroscopic approach, besides t...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Institute of Metals and Materials
سال: 1994
ISSN: 0021-4876,1880-6880
DOI: 10.2320/jinstmet1952.58.5_507