Micro-crack Initiation Life and Micro-fractographic Analysis in Strain Cycling Fatigue of a 60 kg/mm2 High Strength Steel

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Stress- Corrosion Crack Initiation of High-strength Pipeline Steel in Near-neutral pH Environments

Stress-corrosion cracking (SCC) tests were conducted in the near-neutral pH standard solution, NS4, and in an actual soil solution, using four-point bending at a high stress ratio and low frequency conditions very similar to those of operational pipelines. Pitting incubation appeared first and then pitting initiated and grew in both solutions although there were many more pits on the specimen t...

متن کامل

response articles: micro and macro analysis

the present study reports an analysis of response articles in four different disciplines in the social sciences, i.e., linguistics, english for specific purposes (esp), accounting, and psychology. the study has three phases: micro analysis, macro analysis, and e-mail interview. the results of the micro analysis indicate that a three-level linguistic pattern is used by the writers in order to cr...

15 صفحه اول

Side Effects of Shot Peening on Fatigue Crack Initiation Life

Shot peening beneficial effects on fatigue life of mechanical components are well known. However, there are some reports in the literature that indicate inappropriate shot peening parameters tend to reduce the fatigue life. It is therefore, the purpose of this study to find a logical quantitative justification for these observations. Using finite element method, a dynamic elastic-plastic simula...

متن کامل

stress- corrosion crack initiation of high-strength pipeline steel in near-neutral ph environments

stress-corrosion cracking (scc) tests were conducted in the near-neutral ph standard solution, ns4, and in an actual soil solution, using four-point bending at a high stress ratio and low frequency conditions very similar to those of operational pipelines. pitting incubation appeared first and then pitting initiated and grew in both solutions although there were many more pits on the specimen t...

متن کامل

Plastic strain localization and fatigue micro-crack formation in Hastelloy X

In polycrystalline metals, local deformation heterogeneities induced by the microstructure influence fatigue crack initiation and micro-crack propagation. The localization in plastic strains associated with heterogeneous deformation has been described as a necessary condition and a precursor for the nucleation of fatigue cracks. However, a clear and quantitative assessment of the correlation be...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Naval Architects of Japan

سال: 1970

ISSN: 1884-2070,0514-8499

DOI: 10.2534/jjasnaoe1968.1970.128_a331