Microstructural aspects of fatigue in Ni-base superalloys
نویسندگان
چکیده
منابع مشابه
Microstructural aspects of fatigue in Ni-base superalloys.
Nickel-base superalloys are primarily used as components in jet engines and land-based turbines. While compositionally complex, they are microstructurally simple, consisting of small (50-1000 nm diameter), ordered, coherent Ni(3)(Al,Ti)-type L1(2) or Ni(3)Nb-type DO(22) precipitates (called γ(') and γ(''), respectively) embedded in an FCC substitutional solid solution consisting primarily of Ni...
متن کاملHigh Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملMicrostructure and 3-d Effects in Fretting Fatigue of Ti Alloys and Ni-base Superalloys
Damage and plastic deformation accumulation in fretting fatigue occurs within a depth of a few crystallographic grains. Therefore, more accurate assumptions concerning length scale, damage volume, and the material model are needed to establish a more solid physical foundation necessary for next generation fretting fatigue damage prediction. Major thrusts include: (1) development and implementat...
متن کاملMechanisms of creep deformation in polycrystalline Ni-base disk superalloys
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...
متن کاملDeformation Mechanisms in Ni-base Disk Superalloys at Higher Temperatures
This paper presents results from a research initiative aimed at investigating high temperature creep deformation mechanisms in Ni-base superalloys through a combination of creep experiments, TEM deformation mechanism characterization, and state of the art modeling techniques. The effect of microstructure on dictating creep rate controlling deformation mechanisms was revealed for specimens with ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Philosophical Transactions of the Royal Society A: Mathematical, Physical and Engineering Sciences
سال: 2015
ISSN: 1364-503X,1471-2962
DOI: 10.1098/rsta.2014.0128