Abstract A premature pitting corrosion in seam-welded 3-inch L235 steel pipe was reported to occur after 8 years service. This part of a closed ice water cooling system, where the inlet temperature 6 °C and outlet 11 °C. The present work aimed investigate causes this through metallographic investigations. comprised visual examination internal surfaces microstructural examinations perforation regions (pitting areas) using optical scanning electron microscopy (SEM) with energy dispersive X-ray (EDX) analysis. investigations showed that pits occurred only areas huge number specific micro-voids can be associated excessive presence trapped hydrogen dissolved steel, probably during steelmaking operations.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Probabilistic Pitting Corrosion Risk Assessment of Welded Offshore Steel Pipelines

Steel structures continuously exposed to offshore marine environments are prone to corrosion. This can be of major economic and perhaps of environmental significance. The risk of these scenarios occurring can be assessed using good quality data, good quality corrosion and pitting models and structural reliability assessment. Recently, improved models for the prediction of longer term corrosion ...

متن کامل

IMPROVING PITTING CORROSION OF 304 STAINLESS STEEL BY ELECTROPOLISHING TECHNIQUE

Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...

متن کامل

DETERIORATION OF PITTING CORROSION OF 316 STAINLESS STEEL BY SENSITIZATION HEAT TREATMENT

In this research pitting Corrosion of a sensitized 316 stainless steel was investigated employing potentiodynamic, potentiostatic techniques. Sensitization process was carried out on as-received alloy by submitting the specimen in electric furnace set at 650°Cfor five hours and then the specimen was quenched 25°C water. Potentiodynamic polarization of as received and sensitized specimens in 1M ...

متن کامل

Probability Approach for Prediction of Pitting Corrosion Fatigue Life of Custom 450 Steel

In this study, the pitting type of corrosion growth characteristics, fatigue crack initiation and propagation behavior; axial fatigue tests were carried out on precipitation hardened martensitic Custom 450 steel in the air and 3.5wt% NaCl solution. Using the ratio of the depth to the half-width of the pits; (a/c)= 1.5±0.2 the corrosion pit depth growth law was obtained as a function of stress a...

متن کامل

A Statistical Study on the Effect of Hydrostatic Pressure on Metastable Pitting Corrosion of X70 Pipeline Steel

Hydrostatic pressure effects on pitting initiation and propagation in X70 steel are investigated by evaluating metastable pitting probability using electrochemical methods and immersion corrosion tests in containing chlorine ion solution. Potentiodynamic tests indicated that hydrostatic pressure can decrease the breakdown potential and lead to a reduced transpassivity region. Metastable test re...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Failure Analysis and Prevention

سال: 2022

ISSN: ['1864-1245', '1547-7029']

DOI: https://doi.org/10.1007/s11668-022-01530-6