Abstract This work investigated the electrochemical and aqueous tribological behavior of hot pressed 2205 duplex stainless steel (DSS). DSS sintered composites of different volume percent (% vol) of partially stabilized zirconia (PSZ) was developed using powder metallurgy (PM) technique. Electrochemical behaviour was studied at room temperature, using open circuit potential and potentiody...
متن کاملPhase transformation strengthening of high-temperature superalloys
Decades of research has been focused on improving the high-temperature properties of nickel-based superalloys, an essential class of materials used in the hot section of jet turbine engines, allowing increased engine efficiency and reduced CO2 emissions. Here we introduce a new 'phase-transformation strengthening' mechanism that resists high-temperature creep deformation in nickel-based superal...
متن کاملHigh Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملMicrostructure, Mechanical and Tribological Properties of Oxide Dispersion Strengthened High-Entropy Alloys
A novel metal matrix composite CrMnFeCoNi with Y₂O₃ as reinforcement phase was designed and manufactured by mechanical alloying and spark plasma sintering. After sintering at 900 °C for 5 min, the microstructure consisted of a FCC matrix and Y₂O₃ nanoparticles. The addition of 0.25 wt % Y₂O₃ increased the room temperature tensile strength of the CrMnFeCoNi base from 868 MPa to 1001 MPa, while t...
متن کاملHigh Temperature Oxidation and Corrosion Properties of High Entropy Superalloys
The present work investigates the high temperature oxidation and corrosion behaviour of high entropy superalloys (HESA). A high content of various solutes in HESA leads to formation of complex oxides, however the Cr and Al activities of HESA are sufficient to promote protective chromia or alumina formation on the surface. By comparing the oxidation and corrosion resistances of a Ni-based supera...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Tetsu-to-Hagane
سال: 1989
ISSN: 0021-1575,1883-2954
DOI: 10.2355/tetsutohagane1955.75.9_1580