Microstructural control in hot working of IN-718 superalloy using processing map
                    
                        
                            نویسندگان
                            
                            
                        
                        
                    
                    
                    چکیده
منابع مشابه
Effect of Thermomechanical Working on the Microstructure and Mechanical Properties of Hot Pressed Superalloy Inconel 718
Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...
متن کاملOptimization of Hot Workability in Ti-IF Steel by Using the Processing Map
Processing map for hot working of Ti-IF steel has been developed in the temperature range of 750 to 1100 °C and strain rate of 0.01 to 100 s-1. This map in the austenite region exhibits a single domain with a peak efficiency of 45% occurring at 1025 °C and strain rate of 0.02 s-1. The domain extends over the temperature range of 1000 to 1100 °C and strain rate range of 0.01 to 1 s-1. The true s...
متن کاملInvestigation of Cutting Forces Superalloy Inconel 718
Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...
متن کاملCharacterization of strain induced precipitation in Inconel 718 superalloy
Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...
متن کاملoptimization of hot workability in ti-if steel by using the processing map
processing map for hot working of ti-if steel has been developed in the temperature range of 750 to 1100 °cand strain rate of 0.01 to 100 s-1. this map in the austenite region exhibits a single domain with a peak efficiencyof 45% occurring at 1025 °c and strain rate of 0.02 s-1. the domain extends over the temperature range of 1000to 1100 °c and strain rate range of 0.01 to 1 s-1. the true stre...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Metallurgical and Materials Transactions A
سال: 1994
ISSN: 1073-5623,1543-1940