Microstructure evolution under [110] creep in Ni-base superalloys

نویسندگان

چکیده

Microstructure evolutions in Ni-base superalloys are investigated during [110] creep loading using 3D and 2D phase field simulations. A recently developed model coupled to a crystal plasticity based on dislocation densities is employed. The uses storage-recovery law for the density of each glide system hardening matrix account short-range interactions between dislocations. We show that small misorientations tensile axis strongly modify evolution: rafting observed deviations, as opposed microstructure made rod-like precipitates when performed along perfectly aligned direction. Depending precise direction mechanical load, different obtained accompanied by strong modification macroscopic behavior, explaining variety results experimentally. relative role inhomogeneous anisotropic elastic plastic driving forces also investigated, being main force considered case. In addition, our calculations initial slightly modifies morphology but curve significantly impacted.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

Temperature and Orientation Dependence of Creep Damage of Two Ni-base Superalloys

Both polycrystalline (PC) and directionally-solidified (DS) Ni-base superalloys are commonly applied as turbine materials to primarily withstand creep conditions manifested in either marine-, airor land-based gas turbines components. The thrust for increased efficiency of these systems, however, translates into the need for these materials to exhibit considerable strength and temperature resist...

متن کامل

Microstructure and 3-d Effects in Fretting Fatigue of Ti Alloys and Ni-base Superalloys

Damage and plastic deformation accumulation in fretting fatigue occurs within a depth of a few crystallographic grains. Therefore, more accurate assumptions concerning length scale, damage volume, and the material model are needed to establish a more solid physical foundation necessary for next generation fretting fatigue damage prediction. Major thrusts include: (1) development and implementat...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Materialia

سال: 2021

ISSN: ['1873-2453', '1359-6454']

DOI: https://doi.org/10.1016/j.actamat.2021.116851