Microstructure, mechanical response and fractography of AZ91E/Al2O3 (p) nano composite fabricated by semi solid stir casting method

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Optimization of Microstructure and Mechanical Properties of Al-A360 Produced by Semi-Solid Casting

Semi-Solid Casting (SSM) is a new process that could produce globular structures with mechanical properties. The cooling slope method (CLM) is a one of this process that was employed to produce the A360 feedstock. In this method, The dendritic primary phase in the conventionally cast A356 alloy has transformed into a non-dendritic one. In this paper, The molten alloy with the temperature (PT) o...

متن کامل

Effect of Hexagonal Boron Nitrate on Microstructure and Mechanical Behavior of Al7075 Metal Matrix Composite Producing by Stir Casting Technique

Al7075 alloy reinforced with h-Boron Nitrate (BN) composites were processed by stir casting technique. The produced composite was subjected to microstructural studies using OLYMPUS -BX51M, tensile, hardness, density and wear tests. Tensile strength and hardness were found to increase by 12.8% and 20% respectively due to increased dislocation density with the addition of reinforcement. Microstru...

متن کامل

investigation of mechanical property and microstructure of nanocomposite az31/sic fabricated by friction stir process

the friction stir process (fsp) is a solid state process, which has been used to insert reinforcing particles into the structure of a material to create a composite with improved properties. magnesium is a light structural metal that is increasingly used in the aerospace and automobile industries. in this research, sic nanoparticles were added to az31 alloy using fsp in two overlaps of 100% and...

متن کامل

Influence of Nano Reinforced Particles on the Mechanical Properties of Aluminium Hybrid Metal Matrix Composite Fabricated by Ultrasonic Assisted Stir Casting

During the past few decades, materials design has shifted emphasis to pursue low cost, quality, light weight, environment friendliness, and performance. Aluminium matrix composites are important class of engineering materials used in aerospace, automotive, engineering, defence and other industries because of their lower density, higher specific strength, and better physical and mechanical prope...

متن کامل

The Effect of Heat Treatment on the Microstructure and Mechanical Properties of Al/Al3Zr + Al3Ti In-situ Hybrid Composite Fabricated by Friction Stir Processing

In this research, an in-situ hybrid composite reinforced by Al3Zr and Al3Ti aluminide particles was fabricated by friction stir processing (FSP). The base metal was in the form of a rolled Al 3003-H14 alloy sheet, and zirconium and titanium metal powders were used as the reinforcements. Six passes of FSP were applied. Tensile strength and hardness of the base metal, as well as FSPed samples bef...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Magnesium and Alloys

سال: 2017

ISSN: 2213-9567