This article deals with nanoindentation analysis of welded overlay layer Inconel 625 alloy on 16Mo3 steel and their interface (transition zone). The microstructure weld metal is analyzed, as well the weld-on subsequently properties (nanohardnes, reduced modulus elastic-ity) selected structural components. realized a tube made steel, which bent by so-called critical bending (d≤0,7D). also change investigated after that bending. samples prepared from areas highest compressive tensile load outer, respectively inner bend arc were used for research. Nanoindentation was performed using Hysitron Triboin-denter TI950 its evaluation software Triboscan.
منابع مشابه
Laser clading of Inconel 625 on ASTM A575 steel
In this research, the microstructure of Inconel 625 cladded layer on ASTM A575 steel has been investigated. By examining different parameters, the optimal single-pass sample with the least amount of dilution, porosity and fusion and suitable wetting angle was determined. Then cladding process with the optimal parameter was performed. The microstructure of the cladding layer was evaluated from t...
متن کاملLaser clading of Inconel 625 on ASTM A575 steel
In this research, the microstructure of Inconel 625 cladded layer on ASTM A575 steel has been investigated. By examining different parameters, the optimal single-pass sample with the least amount of dilution, porosity and fusion and suitable wetting angle was determined. Then cladding process with the optimal parameter was performed. The microstructure of the cladding layer was evaluated from t...
متن کاملI / RESIDUAL STRESS DISTRIBUTION IN FeAl WELD OVERLAY ON STEEL
Neutron diffraction was used to measure the residual stress distribution in an FeAl weld overlay on steel. It was found that the residual stresses accumulated during welding were essentially removed by the post-weld heat treatment that was applied to the specimen; most residual stresses in the specimen developed during cooling following the post-weld heat treatment. The experimental data were c...
متن کاملInvestigation on the Effect of Post Weld Heat Treatment Temperature on Stress Corrosion Resistance of Inconel 625 Cladded on AISI 4130 Steel Using Hot Wire GTAW
In this research the effect of heat treatment offer welding (PWHT) in 650,750 and 8500C for two hours on Sulfide stress corrosion cracking resistance (SSC), welding metal Inconel 625 to low alloy steel 4130 was analyzed that was welded using Automatic TIG welding process then the mechanical properties of the joint was observed using micro hardness measure experiment (weld metal, base metal and...
متن کاملInvestigation on the Effect of Post Weld Heat Treatment Temperature on Stress Corrosion Resistance of Inconel 625 Cladded on AISI 4130 Steel Using Hot Wire GTAW
In this research the effect of heat treatment offer welding (PWHT) in 650,750 and 8500C for two hours on Sulfide stress corrosion cracking resistance (SSC), welding metal Inconel 625 to low alloy steel 4130 was analyzed that was welded using Automatic TIG welding process then the mechanical properties of the joint was observed using micro hardness measure experiment (weld metal, base metal and...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Manufacturing Technology
سال: 2022
ISSN: ['1213-2489', '2787-9402']
DOI: https://doi.org/10.21062/mft.2022.013