Nanoindentation characterization of nanocomposites coating based on graphene and siloxane matrix deposited by dielectric barrier discharge plasma

نویسندگان

چکیده

Hexamethyldisiloxane (HMDSO)/Graphene nanosheets (GNs) nanocomposite coatings were deposited by a dielectric barrier discharge at atmospheric pressure. Commercially available GNs incorporated into HMDSO precursor different concentrations up to 2 wt%. The analyzed using scanning electron microscopy (SEM) and nanoindentation test. Based on SEM images, it was found that the well distributed dispersed in plasma polymerized hexamethyldisiloxane (ppHMDSO) matrix with no significant agglomeration. results of tests performed continuous stiffness measurements mode showed an increase hardness reduced Young's modulus graphene percentage. maximum two orders magnitude for 2% GNs/ppHMDSO compared homopolymer ppHMDSO. Furthermore, creep compliance analysis exhibited viscoelastic behavior polymer homopolymer.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Surface Decontamination by Dielectric Barrier Discharge Plasma

Background: Dielectric barrier discharge (DBD), a source of non-thermal plasma, is used in surface decontamination. Objective: To study the effect of DBD plasma treatment, we evaluated the effect of plasma exposure time on inactivation of Bacillus subtilis. Results: Applying the DBD plasma to the culture of B. subtilis caused complete sterilization of the surface without any thermal effects. In...

متن کامل

surface decontamination by dielectric barrier discharge plasma

background: dielectric barrier discharge (dbd), a source of non-thermal plasma, is used in surface decontamination. objective: to study the effect of dbd plasma treatment, we evaluated the effect of plasma exposure time on inactivation of bacillus subtilis. results: applying the dbd plasma to the culture of b. subtilis caused complete sterilization of the surface without any thermal effects. in...

متن کامل

Spectroscopic Study of Plasma Polymerized a-C:H Films Deposited by a Dielectric Barrier Discharge

Plasma polymerized a-C:H thin films have been deposited on Si (100) and aluminum coated glass substrates by a dielectric barrier discharge (DBD) operated at medium pressure using C₂Hm/Ar (m = 2, 4, 6) gas mixtures. The deposited films were characterized by Fourier transform infrared reflection absorption spectroscopy (FT-IRRAS), Raman spectroscopy, and ellipsometry. FT-IRRAS revealed the presen...

متن کامل

Modeling of Dielectric Barrier Discharge Plasma Actuator

Glow discharge at atmospheric pressure using a dielectric barrier discharge can induce fluid flow, and operate as an actuator for flow control. In this paper, we simulate the physics of a 2-D asymmetric actuator operating in Helium gas using a high-fidelity first principles-based numerical modeling approach to help improve our understanding of the physical mechanisms associated with such actuat...

متن کامل

Dielectric Barrier Discharge (DBD) Plasma Assisted Synthesis of Ag2O Nanomaterials and Ag2O/RuO2 Nanocomposites

Figure S1a,b show the optical and field emission scanning electron microscope (FESEM) images of the RuO2 NMs. The nanomaterials exhibited nanosheet morphology with length >1 μm and the width <100 nm. The X-ray diffraction (XRD) spectrum (Figure S1c) showed the prominent peaks at the diffraction angle (2θ) 28.00, 34.93, 39.64 and 54.00, representing (110), (101), (200) and (211) set of latti...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Surfaces and Interfaces

سال: 2022

ISSN: ['2468-0230']

DOI: https://doi.org/10.1016/j.surfin.2022.102093