Nanometer-scale precipitations in a selective electron beam melted nickel-based superalloy

نویسندگان

چکیده

Abstract The nanometer-scale (nano-scale) microstructural evolution in an additively manufactured Re-free Ni-based superalloy, with single crystal compositions, is investigated through field emission scanning electron microscopy, transmission and atom probe tomography. We find that nano-scale primary ?? precipitation occurs the fine as-built microstructure, leading to exceptional microhardness of 480.0 ± 6.7 HV at room temperature. Presence ultra-fine precipitates, ~ 20 nm size, observed bottom few layers samples, which hitherto undocumented contrary widespread consensus regarding hierarchical phase superalloys. Moreover, considerable tantalum-rich C14 Laves grain boundaries interdendritic regions samples emphasizes need for additive manufacturing specific alloy design.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

In vivo performance of selective electron beam-melted Ti-6Al-4V structures.

Highly porous titanium structures are widely used for maxillofacial and orthopedic surgery because of their excellent mechanical properties similar to those of human bone and their facilitation of bone ingrowth. In contrast to common methods, the generation of porous titaniumproducts by selective electron beam melting (SEBM), an additive manufacturing technology, overcomes difficulties concerni...

متن کامل

Structural Integrity of an Electron Beam Melted Titanium Alloy

Advanced manufacturing encompasses the wide range of processes that consist of "3D printing" of metallic materials. One such method is Electron Beam Melting (EBM), a modern build technology that offers significant potential for lean manufacture and a capability to produce fully dense near-net shaped components. However, the manufacture of intricate geometries will result in variable thermal cyc...

متن کامل

Nanometer-scale solute clustering in aluminum!/nickel!/ytterbium metallic glasses

The transformation sequence of melt-spun Al!/5.2at.% Ni!/6.8at.% Yb is characterized by X-ray diffraction, differential scanning calorimetry (DSC), and atom-probe field-ion microscopy. An isochronal DSC thermogram detects three major exothermic transformation steps, with onset temperatures of 180, 292, and 327 8C, respectively. Atom-probe analyses reveal the evolution of compositional inhomogen...

متن کامل

Transmission Electron Microscopy Sample Preparation of INCONEL 738 Nickel-Base Superalloy

Size, shape, volume fraction and distribution of embedded g/ phase in g phase has direct effect on strength of INCONEL alloy. Microstructure parameters of INCONEL phases are quantified from microstructure images using transmission electron microscopy (TEM). Different TEM sample preparation techniques were used to study INCONEL 738 alloy microstructure for transmission electron micros...

متن کامل

Approaching the resolution limit of nanometer-scale electron beam-induced deposition.

We report the writing of very high resolution tungsten containing dots in regular arrays by electron beam-induced deposition (EBID). The size averaged over 100 dots was 1.0 nm at fwhm. Because of the statistical spread in the dot size, large and small dots are present in the arrays, with the smallest having a diameter of only 0.7 nm at fwhm. To date these are the smallest features fabricated by...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Scripta Materialia

سال: 2021

ISSN: ['1359-6462', '1872-8456']

DOI: https://doi.org/10.1016/j.scriptamat.2020.113661