Observation of stress corrosion cracking using real-time in situ high-speed atomic force microscopy and correlative techniques
نویسندگان
چکیده
Abstract Contact-mode high-speed atomic force microscopy (HS-AFM) has been utilised to measure in situ stress corrosion cracking (SCC) with nanometre resolution on AISI Type 304 stainless steel an aggressive salt solution. SCC is important failure mode many metal systems but a complicated mechanism that makes difficult predict. Prior the experiments, contributions of microstructure, environment and were independently studied using HS-AFM. During measurements, uplift grain boundaries before was observed, indicating subsurface contribution mechanism. Focussed ion beam milling revealed network intergranular cracks below surface lined thin oxide, process dominated by local at oxide-weakened boundaries. Subsequent analysis atom probe tomography crack tip showed layered oxide composition walls. Oxide formation posited be mechanistically linked boundary uplift. This study shows how HS-AFM observations combination complementary techniques can give insights into mechanisms SCC.
منابع مشابه
High-speed atomic force microscopy.
High-speed atomic force microscopy (HS-AFM) has been developed as a nano-dynamics visualization technique. This microscopy permits direct observation of structure dynamics and dynamic processes of biological molecules in physiological solutions, at a subsecond to sub-100 ms temporal resolution and an ∼2 nm lateral and a 0.1 nm vertical resolution. Importantly, tip-sample interactions do not dis...
متن کاملComponents for high speed atomic force microscopy.
Many applications in materials science, life science and process control would benefit from atomic force microscopes (AFM) with higher scan speeds. To achieve this, the performance of many of the AFM components has to be increased. In this work, we focus on the cantilever sensor, the scanning unit and the data acquisition. We manufactured 10 microm wide cantilevers which combine high resonance ...
متن کاملHigh-speed cycloid-scan atomic force microscopy.
A key hurdle in achieving high scan speeds in atomic force microscopes is that the probe is required to be scanned over the sample in a zig-zag raster pattern. The fast axis of the AFM scanner must track a signal that contains frequencies beyond its mechanical bandwidth. Consequently, fast raster scans generate distortions in the resulting image. We propose a smooth cycloid-like scan pattern th...
متن کاملProgress in the Correlative Atomic Force Microscopy and Optical Microscopy
Atomic force microscopy (AFM) has evolved from the originally morphological imaging technique to a powerful and multifunctional technique for manipulating and detecting the interactions between molecules at nanometer resolution. However, AFM cannot provide the precise information of synchronized molecular groups and has many shortcomings in the aspects of determining the mechanism of the intera...
متن کاملImaging stability in force-feedback high-speed atomic force microscopy.
We studied the stability of force-feedback high-speed atomic force microscopy (HSAFM) by imaging soft, hard, and biological sample surfaces at various applied forces. The HSAFM images showed sudden topographic variations of streaky fringes with a negative applied force when collected on a soft hydrocarbon film grown on a grating sample, whereas they showed stable topographic features with posit...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: npj Materials degradation
سال: 2021
ISSN: ['2397-2106']
DOI: https://doi.org/10.1038/s41529-020-00149-y