Nano-indentation instrumented tests are carried out at shallow depths on PAN-based and MPP-based carbon fibres. Indentation moduli obtained by performing the ten different measured orientations with respect to fibre axis. They used identify elastic constants of fibres, assuming a transversely isotropic behaviour, minimising cost function between estimated values. Inconstancies identified in-plane shear transverse reported literature values pointed out, some drawbacks nano-indentation method highlighted. An improved taking into account buckling mechanisms crystallites stake during indentation process, visible in hysteretic behaviour force-penetration nanoindentation curves, is proposed. It allows that accordance These properties fibres turn estimate epoxy matrix composites containing these Very good agreement found experimentally available unidirectional ply properties. excellent correlation experiments Finite Element Analyses response eventually found.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

the washback effect of discretepoint vs. integrative tests on the retention of content in knowledge tests

در این پایان نامه تاثیر دو نوع تست جزیی نگر و کلی نگر بر به یادسپاری محتوا ارزیابی شده که نتایج نشان دهندهکارایی تستهای کلی نگر بیشتر از سایر آزمونها است

15 صفحه اول

the role of task-based techniques on the acquisition of english language structures by the intermediate efl students

this study examines the effetivenss of task-based activities in helping students learn english language structures for a better communication. initially, a michigan test was administered to the two groups of 52 students majoring in english at the allameh ghotb -e- ravandi university to ensure their homogeneity. the students scores on the grammar part of this test were also regarded as their pre...

15 صفحه اول

investigation of effective parameters on the rigidity of light composite diaphragms (psscb) by fem

در این رساله با معرفی سقف های psscb متشکل از ترکیب ورق های فولادی ذوزنقه ای و تخته های سیمانی الیافی به عنوان سقف های پیش ساخته (سازگار با سیستم سازه ای قاب های فولادی سبک) به بررسی پارامترهای موثر بر صلبیت سقف، پرداخته می شود. در تحقیق حاضر ابتدا به مدل سازی دو نمونه سقف آزمایش شده، به روش اجزاء محدود با استفاده از نرم افزار تحلیلی abaqus ver 6.10 پرداخته شده است. نمونه های ساخته شده تحت اعما...

study of cohesive devices in the textbook of english for the students of apsychology by rastegarpour

this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...

the effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)

cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Carbon

سال: 2021

ISSN: ['0008-6223', '1873-3891']

DOI: https://doi.org/10.1016/j.carbon.2020.09.052