On the stress and temperature dependence of low temperature and high stress shear creep in Ni-base single crystal superalloys
نویسندگان
چکیده
منابع مشابه
High Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملTemperature and Orientation Dependence of Creep Damage of Two Ni-base Superalloys
Both polycrystalline (PC) and directionally-solidified (DS) Ni-base superalloys are commonly applied as turbine materials to primarily withstand creep conditions manifested in either marine-, airor land-based gas turbines components. The thrust for increased efficiency of these systems, however, translates into the need for these materials to exhibit considerable strength and temperature resist...
متن کاملMechanisms of creep deformation in polycrystalline Ni-base disk superalloys
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...
متن کاملModeling the Temperature-dependence of Tertiary Creep Damage of a Directionally Solidified Ni-base Superalloy
Directionally solidified (DS) Ni-base superalloys have become a commonly used material in gas turbine components. Controlled solidification during the material manufacturing process leads to a special alignment of the grain boundaries within the material. This alignment results in different material properties dependent on the orientation of the material. When used in gas turbine applications t...
متن کاملThe Effect of High Temperature Air Exposure on the Stress Rupture Life of Nickel and Cobalt Base Superalloys
The effect of prior air exposure on rupture life of superalloys is reported. Oxygen is identified as a damaging species leading to severe losses in both rupture life and ductility. Similar embrittlement is observed in pure nickel and a mechanism is proposed in terms of reduced grain boundary mobility. Two cobalt base alloys and an oxide dispersion strengthened nickel base alloy do not embrittle...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science and Engineering: A
سال: 2020
ISSN: 0921-5093
DOI: 10.1016/j.msea.2020.139961