Spoof-like plasmonic behavior of plasma enhanced atomic layer deposition grown Ag thin films

The plasmonic behavior of Ag thin films produced by plasma enhanced atomic layer deposition (PEALD) has been investigated. We show that as-deposited flat PEALD Ag films exhibit unexpected plasmonic properties, and the plasmonic enhancement can differ markedly, depending on the microstructure of the Ag film. Electromagnetic field simulations indicate that this plasmonic behavior is due to air ga...

متن کامل

Comparison of ammonia plasma and AlN passivation by plasma-enhanced atomic layer deposition

All material supplied via Aaltodoc is protected by copyright and other intellectual property rights, and duplication or sale of all or part of any of the repository collections is not permitted, except that material may be duplicated by you for your research use or educational purposes in electronic or print form. You must obtain permission for any other use. Electronic or print copies may not ...

متن کامل

Mechanical properties of atomic layer deposition-reinforced nanoparticle thin films.

Nanoparticle thin films (NTFs) exhibit multifunctionality, making them useful for numerous advanced applications including energy storage and conversion, biosensing and photonics. Poor mechanical reliability and durability of NTFs, however, limit their industrial and commercial applications. Atomic layer deposition (ALD) represents a unique opportunity to enhance the mechanical properties of NT...

متن کامل

Atomic layer deposition and properties of ZrO2/Fe2O3 thin films

Thin solid films consisting of ZrO2 and Fe2O3 were grown by atomic layer deposition (ALD) at 400 °C. Metastable phases of ZrO2 were stabilized by Fe2O3 doping. The number of alternating ZrO2 and Fe2O3 deposition cycles were varied in order to achieve films with different cation ratios. The influence of annealing on the composition and structure of the thin films was investigated. Additionally, ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films

سال: 2012

ISSN: 0734-2101,1520-8559

DOI: 10.1116/1.3687937