Optimization of investment casting process for K477 superalloy aero-engine turbine nozzle by simulation and experiment

نویسندگان

چکیده

In order to reduce the shrinkage porosity of nickel-based superalloy castings in investment casting process, effects different gating systems on mold filling, solidification and prediction aero-engine turbine nozzle were investigated by simulation experimental methods. Results show that design vertical runner would cause greater turbulence melt riser during filling outer is not necessary. With decrease number runners, hot spot moves down towards casting, defects are formed below riser. original designs, a certain tendency defect found vanes, inner rings, rings both experiment. Finally, based processing optimization, with no obtained.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Numerical Simulation and Optimization of Directional Solidification Process of Single Crystal Superalloy Casting

The rapid development of numerical modeling techniques has led to more accurate results in modeling metal solidification processes. In this study, the cellular automaton-finite difference (CA-FD) method was used to simulate the directional solidification (DS) process of single crystal (SX) superalloy blade samples. Experiments were carried out to validate the simulation results. Meanwhile, an i...

متن کامل

Optimization of the Investment Casting Process

Rapid prototyping is an important technique for manufacturing. This work refers to the manufacture of hollow patterns made of polymeric materials by rapid prototyping technologies for its use in the preparation of ceramic molds in the investment casting process. This work is focused on the development of a process for manufacturing patterns diff erent from those that currently exist due to its ...

متن کامل

Numerical Simulation of the Investment Casting Process

Determining alloy shrinkage factors is very important for the investment casting process. Casting dimensions can be obtained from numerical simulations of heat transfer and deformation phenomena. The accuracy of the dimensional results depends on heat transfer results. In order to validate heat transfer models, temperature data were obtained during casting of aluminum alloy A356 in shell molds ...

متن کامل

Optimization of Dimensional Deviations in Wax Patterns for Investment Casting

Investment casting is a versatile manufacturing process to produce high quality parts with high dimensional accuracy. The process begins with the manufacture of wax patterns. The dimensional accuracy of the model affects the quality of the finished part. The present study investigated the control and optimization of dimensional deviations in wax patterns. A mold for an H-shaped wax pattern was ...

متن کامل

optimization of dimensional deviations in wax patterns for investment casting

investment casting is a versatile manufacturing process to produce high quality parts with high dimensional accuracy. the process begins with the manufacture of wax patterns. the dimensional accuracy of the model affects the quality of the finished part. the present study investigated the control and optimization of dimensional deviations in wax patterns. a mold for an h-shaped wax pattern was ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: China Foundry

سال: 2022

ISSN: ['1672-6421', '2365-9459']

DOI: https://doi.org/10.1007/s41230-022-1092-4