In this study, a kind of Ni-based superalloy specially designed for additive manufacturing (AM) was investigated. Thermo-Calc simulation and differential scanning calorimetry (DSC) analysis were used to determine phases their transformation temperature. Experimental specimens prepared by laser metal deposition (LMD) traditional casting method. Microstructure, phase constitution mechanical properties the alloy characterized electron microscopy (SEM), transmission (TEM), X-ray diffraction (XRD) tensile tests. The results show that contains two basic phases, ?/?’, in addition these at least secondary may be present, such as MC carbides Laves phases. Furthermore, as-deposited has finer dendrite, its mean primary dendrite arm space (PDAS) is about 30–45 ?m, average size ?’ particles 100–150 nm. However, as-cast much larger PDAS 300–500 ?m with even third arms. Correspondingly, displays different behavior processing methods, specimen shows better ultimate stress (1,085.7±51.7 MPa), yield (697±19.5 MPa) elongation (25.8%±2.2%) than specimen. differences are due morphology dendrites, ?’, phase, segregation elements, etc. Such important information would helpful application well new development.
منابع مشابه
Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483
In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...
متن کاملdetermination of some physical and mechanical properties red bean
چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...
15 صفحه اولSynthesis, structure, and mechanical properties of Ni–Al and Ni–Cr–Al superalloy foams
Reticulated nickel foams were alloyed with 8–9 wt% Al or 14–18 wt% Cr and 5–9 wt% Al in a three-step method consisting of (i) gas-phase deposition of Cr and/or Al onto the struts of a pure Ni foam by pack-cementation at 1000 C; (ii) homogenization at 1200 C to remove concentration gradients and to solutionize the alloyed struts; (iii) aging at 900 C to form c0 precipitates within the struts. Th...
متن کاملAn Overview of Additive Manufacturing of Titanium Components by Directed Energy Deposition: Microstructure and Mechanical Properties
The directed energy deposition (DED) process can be employed to build net shape components or prototypes starting from powder or wires, through a layer-by-layer process. This process provides an opportunity to fabricate complex shaped and functionally graded parts that can be utilized in different engineering applications. DED uses a laser as a focused heat source to melt the in-situ delivered ...
متن کاملmodification of nanoclay for improving the physico-mechanical properties of dental adhesives
هدف اصلی این مطالعه تهیه یک سامانه نوین چسب عاجی دندانی بر پایه نانورس پیوند شده با پلی متاکریلیک اسید، نانورس پیوند شده با پلی اکریلیک اسید، مخلوط نانوسیلیکا و نانورس پیوند شده با پلی متاکریلیک اسید، مخلوط نانوسیلیکا و نانورس پیوند شده با پلی اکریلیک اسید و نانورس پیوند شده با کیتوسان اصلاح شده با گلایسیدیل متاکریلات است. پیوند پلی متاکریلیک اسید و پلی اکریلیک اسید بر ری سطح نانورس در حضور و ...
ذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: China Foundry
سال: 2021
ISSN: ['1672-6421', '2365-9459']
DOI: https://doi.org/10.1007/s41230-021-9025-1