Photocatalytic ozonation of 2, 4-dichlorophenoxyacetic acid in water with a new TiO2 fiber

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Photocatalytic ozonation of 2, 4-dichlorophenoxyacetic acid in water with a new TiO2 fiber

More effective techniques are required to mineralize the increasing number of recalcitrant organic contaminants at low concentrations in the water environment using advanced oxidation process. Though relatively new, photocatalytic ozonation (O3/UV/TiO2) is considered superior to ozonation (O3) and photocatalysis (UV/TiO2), due to synergistic effects and use of immobilized TiO2 photocatalysts is...

متن کامل

Microbial decomposition of 2, 4-dichlorophenoxyacetic acid.

ETCHELLS, J. L., COSTILOW, R. N., AND BELL, T. A. 1952 Identification of yeasts from commercial cucumber fermentations in northern brining areas. Farlowia, 4, 249-264. JANSEN, E. F., AND MACDONNELL, L. R. 1945 Influence of methoxyl content of pectic substances on the action of polygalacturonase. Arch. Biochem., 8, 97-112. JANSEN, E. F., MACDONNELL, L. R., AND JANG, R. 1945 Simultaneous actions ...

متن کامل

Management of 2, 4- Dichlorophenoxyacetic Acid Intoxication by Hemodialysis: A Case Report

Background: The herbicide 2, 4-dichlorophenoxyacetic acid (2, 4-D) can cause moderate to lethal poisoning. Although urine alkalization has been recommended as the main treatment, hemodialysis (HD) may be more effective in severe cases. Case: On 24th June 2014, a 53- year-old man ingested a high amount of 40% 2, 4-D. He suffered from mouth and epigastric burning sensation, vomiting and nausea...

متن کامل

High photocatalytic activity of Fe2O3/TiO2 nanocomposites prepared by photodeposition for degradation of 2,4-dichlorophenoxyacetic acid

Two series of Fe2O3/TiO2 samples were prepared via impregnation and photodeposition methods. The effect of preparation method on the properties and performance of Fe2O3/TiO2 for photocatalytic degradation of 2,4-dichlorophenoxyacetic acid (2,4-D) under UV light irradiation was examined. The Fe2O3/TiO2 nanocomposites prepared by impregnation showed lower activity than the unmodified TiO2, mainly...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Environmental Science & Technology

سال: 2007

ISSN: 1735-1472,1735-2630

DOI: 10.1007/bf03325993