Pitting Corrosion Resistance on Clad-Type of Composite Aluminum Alloys

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Characterization of pitting corrosion in aluminum films by light scattering

We report a detailed study of the morphology of pits formed by corrosion of aluminum thin films using an in-plane light scattering technique. We show that the corrosion front of the Al thin film can be treated as a quasi-two-level random rough surface. Based on an elastic diffraction theory, we are able to determine the average depth, the area, and the density of pits, as well as the fractal di...

متن کامل

Pitting Resistance of Pure Fe-17%Cr Alloys: Consequences for Localized Corrosion Modeling

Pitting corrosion was observed on a high purity Fe-17Cr alloy in 0.02M NaCl solution of pH 6.6 at high anodic potential (+ 550 mVISCE). Potentiostatic electrochemical noise measurements were performed, revealing the presence of a characteristic current noise below stable pitting, differing strongly from that observed 011 a series of AISI 430 type 17% Cr stainless steels, with respect to the fre...

متن کامل

Corrosion Resistance of Dental Alloys

Metals and metallic alloys are unavoidable materials in everyday dental use for the making of fillings, cast cores and post systems, individual crowns, implantants’ suprastructures, dentures and orthodontic devices. They still belong to the vital materials in dentistry. Applied alloys in a mouth are exposed to the influence of chemical, biological, mechanical, thermal and electrical forces whic...

متن کامل

THE ROLE OF ALKALINE CLEANING SOLUTIONS AND CL-CONTAINING LUBRICANTS ON PITTING CORROSION IN NiTi ALLOYS

Alkaline cleaning agents are found to react with remnant manufacturing lubricants trapped in surface defects of a NiTi alloy to form Cl-based salts. These sub-surface “reservoirs” may act as nucleation sites for pitting corrosion either latent under ambient conditions, or on exposure to a limited range of high temperatures used to impart pseudoelastic properties in these alloys as part of norma...

متن کامل

Tarnish Resistance, Corrosion and Stress Corrosion Cracking of Gold Alloys

Tarnishing, corrosion and stress corrosion cracking (SeC) of gold alloys are related phenomena. They present problems when they occur in gold jewellery, dental gold alloys and electronic devices. They are exploited, however, in the depletion gilding and finishing of gold jewellery; and in the extraction, refining and fire assaying of gold. There is still much that is not known about these pheno...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: CORROSION ENGINEERING

سال: 1982

ISSN: 0010-9355,1884-1155

DOI: 10.3323/jcorr1974.31.2_91