Plasma enhanced atomic layer deposition of a (nitrogen doped) Ti phosphate coating for improved energy storage in Li-ion batteries

نویسندگان

چکیده

The use of Ti phosphate as a functional coating for Li ion battery electrodes has been investigated, well the effect nitrogen doping on its electrochemical properties. First, previous knowledge PE-ALD (using an exposure sequence trimethylphosphate plasma–oxygen plasma–titaniumisopropoxide) was used to study altered process using plasma, i.e. TMP* - N2* TTIP. This enabled deposition doped (6 at.%) with growth per cycle 0.4 nm/cycle. Next, dual-source precursor (diethylphosphoramidate or DEPA*) introduced instead TMP*, allowing higher rate (0.6 nm/cycle) and level (8.6 at.%). ionic transparency slightly decreased due incorporation, but effective transversal electronic conductivity showed be three times after doping. A 2 nm (un)doped significantly improved capability lithium nickel manganese cobalt oxide (NMC) electrode, increasing amount energy that can stored at high (dis)charging speeds factor 10 (at 5C). In addition, undoped titanium offered increased stability, retaining 84% capacity 100 cycles 1C respect 79% uncoated electrode.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Ultrathin direct atomic layer deposition on composite electrodes for highly durable and safe Li-ion batteries.

In order to employ Li-ion batteries (LIBs) in next-generation hybrid electric and/or plug-in hybrid electric vehicles (HEVs and PHEVs), LIBs must satisfy many requirements: electrodes with long lifetimes (fabricated from inexpensive environmentally benign materials), stability over a wide temperature range, high energy density, and high rate capability. Establishing long-term durability while o...

متن کامل

Recent Progresses and Development of Advanced Atomic Layer Deposition towards High-Performance Li-Ion Batteries

Electrode materials and electrolytes play a vital role in device-level performance of rechargeable Li-ion batteries (LIBs). However, electrode structure/component degeneration and electrode-electrolyte sur-/interface evolution are identified as the most crucial obstacles in practical applications. Thanks to its congenital advantages, atomic layer deposition (ALD) methodology has attracted enorm...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Ion-Doped Silicate Bioceramic Coating of Ti-Based Implant

Titanium and its alloy are known as important load-bearing biomaterials. The major drawbacks of these metals are fibrous formation and low corrosion rate after implantation. The surface modification of biomedical implants through various methods such as plasma spray improves their osseointegration and clinical lifetime. Different materials have been already used as coatings on biomedical implan...

متن کامل

Ion-Doped Silicate Bioceramic Coating of Ti-Based Implant

Titanium and its alloy are known as important load-bearing biomaterials. The major drawbacks of these metals are fibrous formation and low corrosion rate after implantation. The surface modification of biomedical implants through various methods such as plasma spray improves their osseointegration and clinical lifetime. Different materials have been already used as coatings on biomedical implan...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Power Sources

سال: 2021

ISSN: ['1873-2755', '0378-7753']

DOI: https://doi.org/10.1016/j.jpowsour.2021.229866