Plasma-enhanced atomic layer deposition of silicon nitride for front-end-of-line applications

نویسندگان

چکیده

SiN deposition at low temperatures using the plasma-enhanced atomic layer (PEALD) process is gaining momentum. A high-quality deposited a lower thermal budget and wet etch rates are desired for front-end-of-line applications in semiconductor industries. In this study, of PEALD investigated by utilizing highly reactive trisilylamine silicon precursor three different reaction partners nitrogen precursor. The quality layers compared with reference standard, low-pressure chemical vapor layers. properties interpreted FTIR XPS material characterization techniques. Furthermore, as-deposited annealed investigated. Finally, conformality assessed trench horizontal high aspect ratio structures.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Plasma Deposition of Silicon Nitride

This paper reports on the preparation and characterization of thin films of silicon nitride deposited on heated silicon substrates from Si(CH, ),-NHS-H, mixtures activated at room temperature by an a-c. discharge at low frequency. The films were deposited at 800°C. Deposition rate as well as refractive index were measured and several parameters were systematically varied , including deposition ...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Growth front roughening in silicon nitride films by plasma-enhanced chemical vapor deposition

The dynamic roughening of amorphous silicon nitride growth front prepared by a plasma-enhanced chemical vapor deposition is presented. Morphology of the films grown at different substrate temperatures ~from 50 to 350 °C! for various lengths of deposition time was measured ex situ using atomic force microscopy. The dynamic scaling exponents are measured as a;0.77, b;0.40, and 1/z;0.28, and do no...

متن کامل

Large-scale synthesis of uniform hexagonal boron nitride films by plasma-enhanced atomic layer deposition

Hexagonal boron nitride (h-BN) has been previously manufactured using mechanical exfoliation and chemical vapor deposition methods, which make the large-scale synthesis of uniform h-BN very challenging. In this study, we produced highly uniform and scalable h-BN films by plasma-enhanced atomic layer deposition, which were characterized by various techniques including atomic force microscopy, tr...

متن کامل

Template-Based Synthesis of Aluminum Nitride Hollow Nanofibers Via Plasma-Enhanced Atomic Layer Deposition

Aluminum nitride (AlN) hollow nanofibers were synthesized via plasma-enhanced atomic layer deposition using sacrificial electrospun polymeric nanofiber templates having different average fiber diameters (~70, ~330, and ~740 nm). Depositions were carried out at 200°C using trimethylaluminum and ammonia precursors. AlN-coated nanofibers were calcined subsequently at 500°C for 2 h to remove the sa...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of vacuum science & technology

سال: 2023

ISSN: ['2327-9877', '0734-211X']

DOI: https://doi.org/10.1116/6.0002424