Quinizarin: a large aromatic molecule well suited for atomic layer deposition

نویسندگان

چکیده

Quinizarin is a well-suited molecule for obtaining strongly colored materials by atomic layer deposition.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic Layer Deposition of TiO

Additional resources and features associated with this article are available within the HTML version: • Supporting Information • Links to the 4 articles that cite this article, as of the time of this article download • Access to high resolution figures • Links to articles and content related to this article • Copyright permission to reproduce figures and/or text from this article High surface a...

متن کامل

Fine tuning of nanopipettes using atomic layer deposition for single molecule sensing.

Nanopipettes are an attractive single-molecule tool for identification and characterisation of nucleic acids and proteins in solutions. They enable label-free analysis and reveal individual molecular properties, which are generally masked by ensemble averaging. Having control over the pore dimensions is vital to ensure that the dimensions of the molecules being probed match those of the pore fo...

متن کامل

Atomic layer deposition of ZnS nanotubes.

We report on the growth of high-aspect-ratio (approximately > 300) zinc sulfide nanotubes with variable, precisely tunable, wall thicknesses and tube diameters into highly ordered pores of anodic alumina templates by atomic layer deposition (ALD) at temperatures as low as 75 degrees C. Various characterization techniques are employed to gain information on the composition, morphology and crysta...

متن کامل

Atomic Layer Deposition of Aluminum Oxide

I Acknowledgements II Dedication III List of Figures V

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Dalton Transactions

سال: 2021

ISSN: ['1477-9234', '1477-9226']

DOI: https://doi.org/10.1039/d1dt00683e