Refining of High Purity Ni-base Superalloy Using Calcia Refractory
نویسندگان
چکیده
منابع مشابه
Creep Crack Growth Simulation of Ni-base Superalloy
The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...
متن کاملThermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...
متن کاملDevelopment of a Refractory High Entropy Superalloy
Microstructure, phase composition and mechanical properties of a refractory high entropy superalloy, AlMo0.5NbTa0.5TiZr, are reported in this work. The alloy consists of a nano-scale mixture of two phases produced by the decomposition from a high temperature body-centered cubic (BCC) phase. The first phase is present in the form of cuboidal-shaped nano-precipitates aligned in rows along <100>-t...
متن کاملVery High Cycle Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy DZ4
The effect of casting pores on the very high cycle fatigue (VHCF) behavior of a directionally solidified (DS) Ni-base superalloy DZ4 is investigated. Casting and hot isostatic pressing (HIP) specimens were subjected to very high cycle fatigue loading in an ambient atmosphere. The results demonstrated that the continuously descending S-N curves were exhibited for both the casting and HIP specime...
متن کاملFormation Mechanism of Silicon Modified Aluminide Coating on a Ni-Base Superalloy
Formation mechanism of silicon modified aluminide coating applied on a nickel base super alloy IN-738 LC by pack cementation process was the subject of investigation in this research. Study of the microstructure and compositions of the coating was carried out, using optical and scanning electron microscopes, EDS and X-ray diffraction (XRD) techniques. The results showed that due to low partial ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Tetsu-to-Hagane
سال: 1987
ISSN: 0021-1575,1883-2954
DOI: 10.2355/tetsutohagane1955.73.14_1691