Selective Extraction of Ni from Superalloy Scraps by Molten Mg-Zn

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Adsorption of Zn (II) from aqueous solution by using chitin extraction from crustaceous shell

Removal of toxic heavy metals from wastewater is an important environmental challenge. In this Study, Zn (II) removal from aqueous solution by chitin extraction from crustaceous shells (shrimp and crab) was investigated. The biosorption studies were determined as a function of contact time, pH, initial metal concentration, and the amount of adsorbent. Adsorption of Zn (II) increased with decrea...

متن کامل

Creep of Ni-Al and Ni-Cr-Al Superalloy Foams

The steady-state creep rate of Ni-base metallic foams, with superalloy composition (in wt. pct) Ni7.8∼9.1Al (relative density, ρ = 2.5-2.6) and Ni-13.5∼16.6Cr-5.1∼8.9Al (ρ = 2.8∼3.0), was measured under a range of temperatures (680∼825°C) and applied stresses (0.1∼0.3 MPa), and compared with that of NiAl intermetallic foams (ρ = 5.3). The stress exponent and activation energy are within the exp...

متن کامل

Selective and Efficient Solvent Extraction of Copper(II) Ions from Chloride Solutions by Oxime Extractants

Oxime extractants 3-tert-butyl-2-hydroxy-5-methyl benzaldehyde oxime (HL1) and 3-tert-butyl-2-hydroxy-5-methoxy benzaldehyde oxime (HL2) were synthesized and characterized by conventional spectroscopic methods. Suitable lipophilic nature of the prepared extractants allowed examining the ability of these molecules for extr...

متن کامل

Electroplating and characterization of Zn–Ni, Zn–Co and Zn–Ni–Co alloys

a r t i c l e i n f o Zn–Ni, Zn–Co and Zn–Ni–Co coatings were electrodeposited on mild steel from an acidic chloride bath containing p-aminobenzenesulphonic acid (SA) and gelatin. These additives changed the phase content in the coatings, most likely as a result of their adsorption at the surface of the cathode. The effect of gelatin was more pronounced than that of SA. The Faradaic efficiency ...

متن کامل

Ab initio simulations of molten Ni alloys

Christopher Woodward, Mark Asta, Dallas R. Trinkle, James Lill, and Stefano Angioletti-Uberti Materials and Manufacturing Directorate, Air Force Research Laboratory, Wright Patterson Air Force Base, Dayton, Ohio 45433-7817, USA Department of Materials Science and Engineering, University of California, Berkeley, California 94720, USA and Department of Chemical Engineering and Materials Science, ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2021

ISSN: 2075-4701

DOI: 10.3390/met11060993