Sequential Use of Orthogonal Self‐Assembled Monolayers for Area‐Selective Atomic Layer Deposition of Dielectric on Metal

نویسندگان

چکیده

Although there have been several demonstrations of area-selective atomic layer deposition (AS-ALD) dielectric on in metal/dielectric patterns, the reverse process selective metal (DoM) is not as well developed due to challenge inhibiting only dielectrics. Unavoidable native oxide formation metals tends lead similar surface chemical properties between and substrates, decreasing selectivity inhibitor adsorption. Hence, achieve DoM, preventing unwanted adsorption critical. This study demonstrates a two-step strategy first applying dodecanethiol (DDT) self-assembled monolayer (SAM) Cu/SiO2 pattern protect Cu surfaces from subsequent an octadecyltrimethoxysilane (OTMS) inhibitor, which then selectively forms OTMS SAM SiO2. It further shown that by removing DDT protector with thermal treatment before AS-ALD, ALD growth affected while remains blocked OTMS-covered SiO2 regions. Using this strategy, DoM demonstrated above 0.9 after 5.6 nm ZnO 1.5 Al2O3 ALD. work presents new approach expand material systems available AS-ALD may help enable more applications microelectronics, optoelectronics, energy.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Graphene oxide monolayers as atomically thin seeding layers for atomic layer deposition of metal oxides.

Graphene oxide (GO) was explored as an atomically-thin transferable seed layer for the atomic layer deposition (ALD) of dielectric materials on any substrate of choice. This approach does not require specific chemical groups on the target surface to initiate ALD. This establishes GO as a unique interface which enables the growth of dielectric materials on a wide range of substrate materials and...

متن کامل

GaAs metal-oxide-semiconductor capacitors using atomic layer deposition of HfO2 gate dielectric: Fabrication and characterization

In this letter, we have investigated the physical and electrical characteristics of atomic layer deposition of HfO2 on GaAs substrates. X-ray photoelectron spectroscopy XPS analysis revealed no significant reduction of arsenic oxides upon deposition of HfO2 on GaAs using tetrakis dimethyl-amino hafnium Hf NMe2 4 as the metallic precursor. However, XPS confirmed the absence of arsenic oxides at ...

متن کامل

the use of appropriate madm model for ranking the vendors of mci equipments using fuzzy approach

abstract nowadays, the science of decision making has been paid to more attention due to the complexity of the problems of suppliers selection. as known, one of the efficient tools in economic and human resources development is the extension of communication networks in developing countries. so, the proper selection of suppliers of tc equipments is of concern very much. in this study, a ...

15 صفحه اول

Atomic Layer Deposition of Model Metal Oxide Electrode Architectures

A thorough knowledge of chemical and electrochemical processes that occur at the electrode interface is paramount to the development of improved materials for electrochemical energy storage. One approach is to study model systems with well-defined structures and geometries (architectures) more amenable to systematic and careful study of such materials. The goal of this work is to develop new ap...

متن کامل

Atomic Layer Deposition of Noble Metal Thin Films

3 Preface 4 List of publications 5 List of symbols and abbreviations 6

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Advanced Materials Interfaces

سال: 2022

ISSN: ['2196-7350']

DOI: https://doi.org/10.1002/admi.202202134