Solidification Characteristics and as-Cast Microstructure of Rhenium-Containing Single Crystal Superalloys under High Thermal Gradient Directional Solidification
نویسندگان
چکیده
منابع مشابه
Solidification microstructure development
In the present article, evolution of microstructure during solidification, as a function of various parameters, is discussed. Macrosegregation is described as being due to insufficient diffusivity of solute in the solid. Pattern formation is discussed in the light of instabilities at the solidification growth front. An overview of the scaling relations for various microstructures is given. Meta...
متن کاملDynamical microstructure formation in 3D directional solidification of transparent model alloys: in situ characterization in DECLIC Directional Solidification Insert under diffusion transport in microgravity
To clarify and characterize the fundamental physical mechanisms active in the dynamical formation of three-dimensional (3D) arrays of cells and dendrites under diffusive growth conditions, in situ monitoring of series of experiments on transparent model alloy succinonitrile – 0.24 wt% camphor was carried out under low gravity in the DECLIC Directional Solidification Insert on-board the Internat...
متن کاملNumerical Simulation and Optimization of Directional Solidification Process of Single Crystal Superalloy Casting
The rapid development of numerical modeling techniques has led to more accurate results in modeling metal solidification processes. In this study, the cellular automaton-finite difference (CA-FD) method was used to simulate the directional solidification (DS) process of single crystal (SX) superalloy blade samples. Experiments were carried out to validate the simulation results. Meanwhile, an i...
متن کاملCellular instabilities in directional solidification
2014 We have studied the morphology of the solid-liquid interface during the directional solidification of thin (5-150 03BCm) samples of a dilute binary mixture (CBr4/~ 0.1 % Br2) . Above a critical pulling speed, for a given temperature gradient and solute concentration, the interface, initially planar, breaks down into a periodic cellular pattern. The bifurcation from a planar to a cellular s...
متن کاملSolidification Phenomena and Properties of Some Cast Tool Steels
The freezing process. microstructures and phase relationships in some experimental cast tool steels have been investigated and developed under the various solidification conditions. Experimental steels were based on AISI M2 and M10 grades high speed steels. Addition of carbide forming elements such as niobium and titanium with and without extra carbon were made to the molten bath of the base st...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Advanced Materials Research
سال: 2011
ISSN: 1662-8985
DOI: 10.4028/www.scientific.net/amr.278.423