Spatial atomic layer deposition: A route towards further industrialization of atomic layer deposition
نویسندگان
چکیده
منابع مشابه
Atomic Layer Deposition of TiO
Additional resources and features associated with this article are available within the HTML version: • Supporting Information • Links to the 4 articles that cite this article, as of the time of this article download • Access to high resolution figures • Links to articles and content related to this article • Copyright permission to reproduce figures and/or text from this article High surface a...
متن کاملAtomic layer deposition of ZnS nanotubes.
We report on the growth of high-aspect-ratio (approximately > 300) zinc sulfide nanotubes with variable, precisely tunable, wall thicknesses and tube diameters into highly ordered pores of anodic alumina templates by atomic layer deposition (ALD) at temperatures as low as 75 degrees C. Various characterization techniques are employed to gain information on the composition, morphology and crysta...
متن کاملAtomic Layer Deposition of Aluminum Oxide
I Acknowledgements II Dedication III List of Figures V
متن کاملAtomic layer deposition of transition metals.
Atomic layer deposition (ALD) is a process for depositing highly uniform and conformal thin films by alternating exposures of a surface to vapours of two chemical reactants. ALD processes have been successfully demonstrated for many metal compounds, but for only very few pure metals. Here we demonstrate processes for the ALD of transition metals including copper, cobalt, iron and nickel. Homole...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
سال: 2012
ISSN: 0734-2101,1520-8559
DOI: 10.1116/1.3670745