Specific heat capacity measurement of Phyllostachys edulis (Moso bamboo) by differential scanning calorimetry

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Measurement of Heat Capacity by Differential Scanning Calorimetry

The methods of measuring the heat capacity of materials by differential scanning calorimetry (DSC) are presented and discussed. The principles of temperature modulated DSC are outlined and the possibilities and limits of the method are discussed.

متن کامل

Measurement of Specific Heat Functions by Differential Scanning Calorimetry

When a sample material is subjected to a linear temperature program, the heat flow rate into the sample i s proportional to its instantaneous specific heat. By recording this heat flow rate as a function of temperature, and comparing it with the heat flow rate into a standard material under the same conditions, the specific heat of the sample i s determined as a fundion of temperature. The meth...

متن کامل

Transcriptome Sequencing and Analysis of the Fast Growing Shoots of Moso Bamboo (Phyllostachys edulis)

BACKGROUND The moso bamboo, a large woody bamboo with the highest ecological, economic, and cultural value of all bamboos, has one of the highest growth speeds in the world. Genetic research into moso bamboo has been scarce, partly because of the lack of previous genomic resources. In the present study, for the first time, we performed de novo transcriptome sequencing and mapped to the moso bam...

متن کامل

Genome-wide identification and expression analysis of the IQD gene family in moso bamboo (Phyllostachys edulis).

Members of the plant-specific IQ67-domain (IQD) protein family are involved in various aspects of normal plant growth and developmental processes as well as basal defence response. Although hundreds of IQD proteins have been identified, only a small number of IQDs have been functionally characterized. Moreover, no systematic study has been performed on moso bamboo. In this study, we performed f...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Construction and Building Materials

سال: 2016

ISSN: 0950-0618

DOI: 10.1016/j.conbuildmat.2016.08.103