Stress Corrosion Cracking Behaviour of Dissimilar Welding of AISI 310S Austenitic Stainless Steel to 2304 Duplex Stainless Steel

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Dissimilar Welding of EN 10025 Carbon Steel to AISI 316L Stainless Steel by Friction Stir Welding

In the present Study, a dissimilar joint of carbon steel sheet EN 10025 with 316 L has been welded by FSW and the welding parameters were optimized by RSM software method. For investigation of mechanical properties and microstructural analysis carried out by using optical, scanning electron microscopes with EDS analysis, tensile and hardness test of different area of joints, SZ, TMAZ, HAZ, thei...

متن کامل

Dissimilar Welding of EN 10025 Carbon Steel to AISI 316L Stainless Steel by Friction Stir Welding

In the present Study, a dissimilar joint of carbon steel sheet EN 10025 with 316 L has been welded by FSW and the welding parameters were optimized by RSM software method. For investigation of mechanical properties and microstructural analysis carried out by using optical, scanning electron microscopes with EDS analysis, tensile and hardness test of different area of joints, SZ, TMAZ, HAZ, thei...

متن کامل

Dissimilar resistance spot welding of AISI 1075 eutectoid steel to AISI 201 stainless steel

In this paper, dissimilar resistance spot welding of AISI 1075 eutectoid steel to AISI 201 stainless steel is investigated experimentally. For this purpose, the experiments are designed using response surface methodology and based on four-factor, five-level central composite design. The effects of process parameters such as welding current, welding time, cooling time and electrode force are inv...

متن کامل

Stress Corrosion Cracking of an Austenitic Stainless Steel in Nitrite-Containing Chloride Solutions

This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC) in a nitrite-containing chloride solution. Slow strain rate testing (SSRT) in 30 wt. % MgCl₂ solution established SCC susceptibility, as evidenced by post-SSRT fractography. Addition of nitrite to the chloride solution, which is reported to have inhibitive influence on corrosion of stainless ste...

متن کامل

A Continuum Damage Model for the Stress Corrosion Cracking of Austenitic Stainless Steel

In the present work, the mechanical behavior of stress corrosion cracking phenomenon is described. Such phenomenon presents strong complexity due to metallurgic and electrochemical aspects. A methodology for modeling both SSR (Slow Strain Rate) and CL (Constant Load) tests based upon thermodynamics of continuum solids and elastoplastic damage is proposed. In this macroscopic approach, besides t...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2018

ISSN: 2075-4701

DOI: 10.3390/met8030195