Stress Corrosion Cracking of a SUS304 Stainless Steel in MgCl2 Solution

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution

The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...

متن کامل

In-Situ Observation and Acoustic Emission Analysis for Corrosion Pitting of MgCl2 Droplet in SUS304 Stainless Steel

Acoustic emission with near-field detection and optical video microscope monitoring was proposed to investigate the pitting corrosion caused by a small magnesium-chloride droplet. Four types of the detected waveforms were characterized by the wavelet analysis to investigate the corrosion of work-hardened SUS304 stainless steel. After high-activity AE signals observed, the corrosion product shee...

متن کامل

A Continuum Damage Model for the Stress Corrosion Cracking of Austenitic Stainless Steel

In the present work, the mechanical behavior of stress corrosion cracking phenomenon is described. Such phenomenon presents strong complexity due to metallurgic and electrochemical aspects. A methodology for modeling both SSR (Slow Strain Rate) and CL (Constant Load) tests based upon thermodynamics of continuum solids and elastoplastic damage is proposed. In this macroscopic approach, besides t...

متن کامل

Stress Corrosion Cracking of an Austenitic Stainless Steel in Nitrite-Containing Chloride Solutions

This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC) in a nitrite-containing chloride solution. Slow strain rate testing (SSRT) in 30 wt. % MgCl₂ solution established SCC susceptibility, as evidenced by post-SSRT fractography. Addition of nitrite to the chloride solution, which is reported to have inhibitive influence on corrosion of stainless ste...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1978

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.27.303appendix_1158