Stress Corrosion Cracking of Friction Stir-Welded AA-2024 T3 Alloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue of Friction Stir Welded 2024-T351 Aluminium Alloy

Fatigue failure characteristics of friction stir welds in 13mm gauge 2024-T351 plate have been assessed. Failure occurred from either the weld region (nugget/flow arm) or from the material immediately surrounding the weld. Fatigue failure from the surrounding material was essentially conventional, initiating from large S-phase intermetallic particles and growing in a macroscopic mode I manner. ...

متن کامل

Corrosion Behavior of the Friction Stir Welded AZ31 Magnesium Alloy.

* IDMEC, Instituto Superior Técnico, Universidade de Lisboa, Av. Rovisco Pais, 1049-001 Lisboa, Portugal ** DEQ/ICEMS, Instituto Superior Técnico, Universidade de Lisboa, Av. Rovisco Pais, 1049001 Lisboa, Portugal. *** Department of Engineering Design and Production, School of Engineering, Aalto University, P.O. Box 1420, FI-00076 Aalto, Finland **** Faculdade de Engenharia da universidade do P...

متن کامل

Corrosion behaviour of friction stir welded AZ61A magnesium alloy welds immersed in NaCl solutions

The extruded AZ61A magnesium alloy plates of 6 mm thickness were butt welded using friction stir welding (FSW) process. The corrosion behavior of the welds was evaluated by conducting immersion test in NaCl solution at different pH value, immersion time and chloride ion concentrations. An empirical relationship was established incorporating pH value, immersion time and chloride ion concentratio...

متن کامل

The Mechanical Properties Evaluation of the Welded Sheets of AA 3105 Aluminum Alloy Using Friction Stir Spot Welding (FSSW)

Friction stir spot welding (FSSW) is a type of solid state welding that is used in the connection of small pieces and light metals such as aluminum alloy especially. The technical problem during melting of aluminum alloys is one of the most important reasons for developing application of friction stir welding for aluminum alloys. In this research, the effects of important processing parameters ...

متن کامل

Experimental Investigation of Tensile Strength and Deflection Characteristics of Friction Stir Welded Aluminum AA 6351 Alloy Joint

Aluminum alloys are used in many applications in which the combination of high strength and low weight is attractive; ship building, air frame, transportation industry etc. are some areas in which the low weight can be significant value. Friction stir welding (FSW) is a new welding technique particularly well suited to aluminum alloys though this technique is also used for other materials. Fric...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials

سال: 2020

ISSN: 1996-1944