Stress Corrosion Cracking of Pipeline Steel

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Corrosion Product Film-Induced Stress Facilitates Stress Corrosion Cracking

Finite element analyses were conducted to clarify the role of corrosion product films (CPFs) in stress corrosion cracking (SCC). Flat and U-shaped edge-notched specimens were investigated in terms of the CPF-induced stress in the metallic substrate and the stress in the CPF. For a U-shaped edge-notched specimen, the stress field in front of the notch tip is affected by the Young's modulus of th...

متن کامل

Tarnish Resistance, Corrosion and Stress Corrosion Cracking of Gold Alloys

Tarnishing, corrosion and stress corrosion cracking (SeC) of gold alloys are related phenomena. They present problems when they occur in gold jewellery, dental gold alloys and electronic devices. They are exploited, however, in the depletion gilding and finishing of gold jewellery; and in the extraction, refining and fire assaying of gold. There is still much that is not known about these pheno...

متن کامل

Stress- Corrosion Crack Initiation of High-strength Pipeline Steel in Near-neutral pH Environments

Stress-corrosion cracking (SCC) tests were conducted in the near-neutral pH standard solution, NS4, and in an actual soil solution, using four-point bending at a high stress ratio and low frequency conditions very similar to those of operational pipelines. Pitting incubation appeared first and then pitting initiated and grew in both solutions although there were many more pits on the specimen t...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: CORROSION ENGINEERING

سال: 1974

ISSN: 0010-9355,1884-1155

DOI: 10.3323/jcorr1974.23.6_281