STRESS CORROSION CRACKING SAMBUNGAN LAS CDW SS 316L DAN ASTM A36 DALAM VARIASI SUHU LINGKUNGAN KOROSIF FeCl2

نویسندگان

چکیده

Stress Corrosion Cracking (SCC) is known as a trigger for material failure, especially in Dissimilar Metal Welding (DMW). Although DMW promises wide application structural design, it found that there high SCC mitigation making prone to failure. Capacitor Discharge (CDW) one of the best dissimilar metal welding methods. This article observes weld joints CDW ASTM A36 and SS 316L against phenomenon corrosive environment temperature variation FeCl2 0.5 Molar (30, 40, 50 0C). The results Constant Load Test (CLT) show threshold strength has decreased significantly due increase galvanic corrosion current which increases at temperatures. stress specimen T1 with 30 0C K1cc 360 MPa, T2 produces 216 MPa T3 144 MPa. It can be concluded changes accelerate reaction accelerates occurrence corrosiveness joint. SEM/EDS photo evaluation provides perfect picture distribution fracture surface. At highest 0C, surface rate causes lot bubbles porous pores fracture, this connection weaken.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Corrosion Product Film-Induced Stress Facilitates Stress Corrosion Cracking

Finite element analyses were conducted to clarify the role of corrosion product films (CPFs) in stress corrosion cracking (SCC). Flat and U-shaped edge-notched specimens were investigated in terms of the CPF-induced stress in the metallic substrate and the stress in the CPF. For a U-shaped edge-notched specimen, the stress field in front of the notch tip is affected by the Young's modulus of th...

متن کامل

Tarnish Resistance, Corrosion and Stress Corrosion Cracking of Gold Alloys

Tarnishing, corrosion and stress corrosion cracking (SeC) of gold alloys are related phenomena. They present problems when they occur in gold jewellery, dental gold alloys and electronic devices. They are exploited, however, in the depletion gilding and finishing of gold jewellery; and in the extraction, refining and fire assaying of gold. There is still much that is not known about these pheno...

متن کامل

ARPA Coupling Program on Stress - Corrosion Cracking

A progress report of the ret arch invest carried out on the problem of stress-cor high strength materials under ARPA Order Work at Carnegie-Mellon University, Lehi Georgia Institute of Technology, The Boe American University, and the Naval Resea cerning test techniques, materials chara metallurgy, surface studies, and corrosi described. The report is divided into t covering work on high strengt...

متن کامل

Acoustic Emission during Stress Corrosion Cracking Test

AE monitoring from various types of stress corrosion cracking (SCC) has been conducted for the past 15 years in our laboratory. This paper discusses AE results of active-path dissolution-type SCC of austenitic stainless steel in chloride solution and fused salt, fluoride and polythionic acid solutions, brass in ammonia (Mattosson's solution), and carbon steels in nitrite solution. Transgranular...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Rekayasa Mesin

سال: 2023

ISSN: ['2338-1663', '2477-6041']

DOI: https://doi.org/10.21776/jrm.v13i3.1244