Super-Solidus Hot Isostatic Pressing Heat Treatments for Advanced Single Crystal Ni-Base Superalloys

نویسندگان

چکیده

Abstract Super-solidus hot isostatic pressing (SSHIP) heat treatment has first been developed and applied to the third-generation Ni-base single crystal superalloy CMSX-10 K. This new type of aims at significantly reducing total time required for solution enhancing mechanical properties as compared conventional routes. The SSHIP is an innovative, economical sustainable approach that can be all types SX superalloys. It especially interesting alloys with a high content refractory elements large volume fraction eutectic microstructure in as-cast state.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Neural Observer for the Hot Isostatic Pressing

Hot Isostatic Pressing (HIP'ing) is one of several processes used for consolidating porous materials (such as metal powders) to high density. The equations describing the HIP'ing system dynamics are immensely complicated and highly nonlinear, thus complicating any controller design for the system. Further complications arise due to the fact that one of the system's states, grain size, cannot be...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

Sensing a N D Modeling of the Hot Isostatic Pressing of Copper Pressing

-A detailed experimental evaluation of mathematical models for densification during hot isostatic pressing (HIP) has been conducted using high purity copper powder as a model system. Using a new eddy current sensor, the density of cylindrical compacts has been measured/n situ and compared with model predictions for the HIP process. Pressure shielding by the can has been found to influence the d...

متن کامل

Deformation Mechanisms in Ni-base Disk Superalloys at Higher Temperatures

This paper presents results from a research initiative aimed at investigating high temperature creep deformation mechanisms in Ni-base superalloys through a combination of creep experiments, TEM deformation mechanism characterization, and state of the art modeling techniques. The effect of microstructure on dictating creep rate controlling deformation mechanisms was revealed for specimens with ...

متن کامل

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions

سال: 2022

ISSN: ['1073-5623', '1543-1940']

DOI: https://doi.org/10.1007/s11661-022-06884-y