Susceptibility to Pitting Corrosion of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V Alloys for Aeronautical Applications

نویسندگان

چکیده

Titanium alloys are used in different industries like biomedical, aerospace, aeronautic, chemical, and naval. Those have high requirements with few damage tolerances. Therefore, they necessary to use materials that present fatigue, mechanical, corrosion resistance. Although Ti-alloys material performance, exposed marine industrial environments. This research shows the behavior of three titanium alloys, specifically Ti CP2, Ti-6Al-2Sn-4Zr-2Mo, Ti-6Al-4V. Alloys were on two electrolytes a 3.5 wt % H2SO4 NaCl solutions at room temperature using cyclic potentiodynamic polarization (CPP) electrochemical noise (EN) according ASTM G61 G199 standards. CPP technique was employed obtain parameters as passivation range (PR), type, passive layer persistence, potential (Ecorr), rate. EN analyzed by power spectral density (PSD) voltage. Results obtained revealed pseudopassivation PSD for indicating instability rate lower. However, Ti-6Al-4V presented highest both electrolytes. Ti-6Al-2Sn-4Zr-2Mo NaCl, unstable. lower solutions.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue of Ti-6Al-4V

Metallic biomaterials have essentially three fields of use; these are the artificial hip joints, screw, plates and nails for internal fixation of fractures, and dental implants. Any of these devices must support high mechanical load and resistance of material against breakage is essential. High mechanical properties are needed for structural efficiency of surgical and dental implants. But their...

متن کامل

Notch Corrosion Fatigue Behavior of Ti-6Al-4V

The aim of this paper is to map the corrosion fatigue characteristics of Ti-6Al-4V alloy through the evaluation of the corrosion fatigue initiation and failure mechanisms. The study included the effect of the stress concentration factor at very high Kt values and the role of different inert or corrosive environments. This alloy is widely used in naval-structures and aero-engine communities and ...

متن کامل

Gas nitriding and subsequent oxidation of Ti-6Al-4V alloys

Ti-6Al-4V alloys consisting of α-Ti grains and intergranular β-Ti islands were nitrided at 850°C for 1 to 12 h under a nitrogen pressure of 1 Pa. With increasing nitriding time, the Ti-N compound layer became thicker, and the α-Ti diffusion zone containing dissolved nitrogen became wider. In the Ti-N compound layer, the initially formed Ti2N became TiN as the nitriding progressed. The nitride l...

متن کامل

Biomimetic Hydroxyapatite Growth on Functionalized Surfaces of Ti-6Al-4V and Ti-Zr-Nb Alloys

A biomimetic approach for coating titanium-containing alloys with hydroxyapatite (HA) is reported in the article. Two types of Ti-containing alloys were chosen as an object for coating: Ti-6Al-4V (recommended for orthopedic application) and a novel highly biocompatible Ti-Zr-Nb alloy, with good mechanical compatibility due to a modulus that is more close to that of human bones (E ≈ 50 GPa inste...

متن کامل

Corrosion resistance of Ti-6Al-4V and ASTM F75 alloys processed by electron beam melting

The electron beam melting (EBM) is a useful technique for fabricating alloys that are difficult to machine and require expensive tools as well as the presence of inert atmosphere for further treatments. Under vacuum, EBM provides a controlled environment, reducing the drawbacks of the alloys of their processing in a conventional manner and thereby improving their microstructure, which can enhan...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2021

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met11071002