A suite of experimental tools and fast-acting, numerical-simulation techniques was used to quantify the precipitation behavior three nickel-base superalloys: IN-100, LSHR, 718. Experimental methods comprised differential scanning calorimetry (DSC) establish specific heat as a function temperature selected direct-resistance heating trials (using Gleeble® machine) obtain samples for microstructural analysis. For DSC experiments, each alloy cooled at prescribed constant rate (between 5 20 K/min) after an initial soak/equilibration in high-temperature, single-phase (supersolvus) regime. On-heating beginning ambient were also performed on 718 different starting conditions: super-δ-solvus solution treated water quenched (denoted ST), aged (STA), overaged (STOA). results, revealing thermal signatures associated with kinetics γ′ (IN-100, LSHR) or γ″ (718), interpreted using previously-developed fast-acting routine that treats concurrent nucleation, growth, coarsening, dissolution. these simulations, special attention paid various thermo-kinetic input parameters including equilibrium solvus-approach curves, bulk free energies transformation, matrix-precipitate interface energies, effective diffusivities. γ-γ′ superalloys (IN-100 LSHR), estimates precipitate volume fraction from specific-heat data revealed semi-quantitative agreement simulation predictions. γ-γ′-γ″ superalloy predictions fractions converted showed direct measurements.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Review on Thermo-Mechanical Fatigue Behavior of Nickel-Base Superalloys

Nickel-base superalloys have become the key materials of hot-end components in the aeroengines over the past several decades. Nickelbase superalloys are easy to produce thermo-mechanical fatigue (TMF) behavior when withstanding the combined effects of high temperature, creep, oxidation, mechanical stress and thermal stress. The occurrence of TMF seriously affects the normal service for hot-end ...

متن کامل

Application of Differential Scanning Calorimetry to the Characterization of Biopolymers

Generally, polymers can be classified according to their thermal and mechanical properties into thermoplastics, thermosets and elastomers. Thermoplastics are amorphous or semicrystalline polymers that soft or melt during heating and solidify during cooling. The heating/cooling/heating process can be repeated without perceptible changes in thermal and mechanical properties of thermoplastics. The...

متن کامل

Isothermal titration calorimetry and differential scanning calorimetry as complementary tools to investigate the energetics of biomolecular recognition.

The principles of isothermal titration calorimetry (ITC) and differential scanning calorimetry (DSC) are reviewed together with the basic thermodynamic formalism on which the two techniques are based. Although ITC is particularly suitable to follow the energetics of an association reaction between biomolecules, the combination of ITC and DSC provides a more comprehensive description of the ther...

متن کامل

Evaluation and Characterization of Free and Immobilized Acethylcholinesterase with Fluorescent Probe, Differential Scanning Calorimetry and Docking

Acetylcholinesterase (AChE) enzyme which catalyses the hydrolysis of choline esters, such as acetylcholine, is very important in nerve function. Previous structural studies showed the possible amyloid fibril formation on the AChE. Therefore it is important to understand interaction of ligands to prevent the formation of  amyloid fibrils. The purpose of the present study was to  char...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions

سال: 2021

ISSN: ['1073-5623', '1543-1940']

DOI: https://doi.org/10.1007/s11661-021-06362-x