The Effect of Forging and Heat Treatment Variables on Microstructure and Mechanical Properties of a Re-Bearing Powder-Metallurgy Nickel Base Superalloy

نویسندگان

چکیده

In our previous works, the effects of forging and heat treatment variables on microstructure evolution mechanical properties have been studied for an ingot-metallurgy Re-bearing nickel base superalloy. To overcome issues associated with production large-scale ingots fine-grained workpieces, in present work, effect hot was a superalloy prepared via powder metallurgy. The purpose study to reach properly balanced potential use as disc material. initial as-HIPed workpieces were subjected different post-forging or only (no forging). For processed recrystallization behavior, size, morphology volume fraction γ′ precipitates evaluated by scanning electron microscopy followed properties. most (strength, ductility, creep resistance rupture lifetime) reached γ grain size dγ ≈ 13.6 µm. A finer coarser (down 2.6 up 37.5 µm) even when superimposed higher dispersed secondary (in case = 27–37.5 worse

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Heat Treatment Process on Microstructure and Fatigue Behavior of a Nickel-Base Superalloy

The study of fatigue behaviors for nickel-base superalloys is very significant because fatigue damage results in serious consequences. In this paper, two kinds of heat treatment procedures (Pro.I and Pro.II) were taken to investigate the effect of heat treatment on microstructures and fatigue behaviors of a nickel-base superalloy. Fatigue behaviors were studied through total strain controlled m...

متن کامل

Effects of Friction Stir Process Parameters on Microstructure and Mechanical properties of Aluminum Powder Metallurgy Parts

The effects of friction stir processing (FSP) on the microstructure and mechanical properties of aluminum powder metallurgy (PM) parts was investigated. PM parts were then subjected to FSP at advancing speeds (v) of 40-200 mm/min and tool rotational speeds (ω) of 800-1600 rpm. Microhardness (HV) and tensile tests at room temperature were used to evaluate the mechanical properties of the frictio...

متن کامل

determination of some physical and mechanical properties red bean

چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...

15 صفحه اول

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2023

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met13061110