Thermal and Nanoindentation Behaviours of Layered Silicate Reinforced Recycled GF-12 Nanocomposites

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Polymer Layered Silicate Nanocomposites: A Review

This review aims to present recent advances in the synthesis and structure characterization as well as the properties of polymer layered silicate nanocomposites. The advent of polymer layered silicate nanocomposites has revolutionized research into polymer composite materials. Nanocomposites are organic-inorganic hybrid materials in which at least one dimension of the filler is less than 100 nm...

متن کامل

Polymer- Layered Silicate Nanocomposites for Cryotank Applications

Previous composite cryotank designs have relied on the use of conventional composite materials to reduce microcracking and permeability. However, revolutionary advances in nanotechnology derived materials may enable the production of ultra-lightweight cryotanks with significantly enhanced durability and damage tolerance, as well as reduced propellant permeability. Layered silicate nanocomposite...

متن کامل

Electrospinning of Poly (mma-co-maa) Copolymers and Their Layered Silicate Nanocomposites for Improved Thermal Properties

Copolymers consisting of methyl methacrylate (MMA) and methacrylic acid (MAA) and their layered silicate nanocomposites were electrospun to form fibers with diameters in the sub-micron range. The presence of MAA increased the glass transition temperature and thermal stability of the copolymers through formation of anhydrides upon heating. Dispersion of layered silicates within the nanocomposite...

متن کامل

Polymer-Layered Silicate Nanocomposites: Synthesis, Properties and Applications

Polymer nanocomposites, especially polymerlayered silicate (PLS) nanocomposites, represent a radical alternative to conventionally (macroscopically) filled polymers. Because of their nanometer-size dispersion, the nanocomposites exhibit markedly improved properties when compared with the pure polymers or conventional composites. These include increased modulus and strength, decreased gas permea...

متن کامل

Study on the Optical and Rheological properties of polymer- layered Silicate Nanocomposites

This review reports recent advances in the field of polymer–layered silicate nano composites. Thesematerials have attracted both academic and industrial attention because they exhibit dramaticimprovement in properties at very low filler contents. Herein, the structure, preparation andproperties of polymer–layered silicate nanocomposites are discussed in general, and finally the effectof clay na...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Materials Science Research

سال: 2016

ISSN: 1927-0593,1927-0585

DOI: 10.5539/jmsr.v5n4p10