Thermomechanical model for solidification and cooling simulation of Ni-based superalloy components

نویسندگان

چکیده

One of the challenges encountered in industrialization new single-crystal superalloys parts (like high-pressure turbine blades and vanes for aircraft engines) is to limit mechanical stresses during solidification cooling metal. In order accurately predict viscoplastic flow as well thermo-mechanical behaviour Ni-based superalloy its cooling, this study a thermodynamically-consistent thermo-elasto-viscoplastic model was developed. This takes into account solid-liquid transition occurring material phase. done by introducing compressible-type yield function based on appropriate equivalent stress depending volume fraction solid phase formed propagation dendrites inside liquid material. implemented Abaqus/Standard© F.E. code applied identification parameters using isothermal tensile-relaxation tests driven different strain rates temperatures. First, anisothermal tensile-compression test simulated single integration point. A comparison experimental numerical stress-strain response partially validate model. Second, benchmark involving casting rectangular bar sand mold analyzed.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

In- and Out-of Phase Thermomechanical Fatigue of a Ni-Based Single-Crystal Superalloy

In this study, the difference between in-phase (IP) and out-of-phase (OP) thermomechanical fatigue (TMF) cycling from 100 to 750 ◦C has been investigated for the Ni-based single-crystal superalloy MD2. In addition, two different crystal orientations were studied, the 〈001〉 and 〈011〉 orientations respectively. When comparing IP and OP TMF lives, a strain range dependency is found for the 〈001〉 d...

متن کامل

Directional Solidification Microstructure of a Ni-Based Superalloy: Influence of a Weak Transverse Magnetic Field

A Ni-based superalloy CMSX-6 was directionally solidified at various drawing speeds (5–20 μm·s−1) and diameters (4 mm, 12 mm) under a 0.5 T weak transverse magnetic field. The results show that the application of a weak transverse magnetic field significantly modified the solidification microstructure. It was found that if the drawing speed was lower than 10 μm·s−1, the magnetic field caused ex...

متن کامل

A simple Analytical model for solidification cooling rate based on the local heat flux density

A new simple analytical model for prediction of cooling rate in the solidification process based on the local heat flux density extracted during solidification is introduced. In the modeling procedure, a solidifying control volume is considered in the mushy zone in which a heat balance equation is used to derive the present model. As the local heat flux density is a measurable parameter, the pr...

متن کامل

Effect of Solidification Behavior on Microstructures and Mechanical Properties of Ni-Cr-Fe Superalloy Investment Casting

The effect of solidification behavior on the microstructures and mechanical properties of Ni-Cr-Fe superalloy investment casting is given. Metallographic and image analysis have been used to quantitatively examine the microstructures' evolution. For the parts with the thickness of 3 mm and 24 mm, the volume fraction and maximum equivalent radius of the Laves phase increases from 0.3% to 1.2%, f...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Solids and Structures

سال: 2021

ISSN: ['1879-2146', '0020-7683']

DOI: https://doi.org/10.1016/j.ijsolstr.2020.12.009