TiO2 Nanomembranes Fabricated by Atomic Layer Deposition for Supercapacitor Electrode with Enhanced Capacitance

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atomic layer deposition of Co3O4 on carbon nanotubes/carbon cloth for high-capacitance and ultrastable supercapacitor electrode.

Co3O4 nanolayers have been successfully deposited on a flexible carbon nanotubes/carbon cloth (CC) substrate by atomic layer deposition. Much improved capacitance and ultra-long cycling life are achieved when the CNTs@Co3O4/CC is tested as a supercapacitor electrode. The improvement can be from the mechanically robust CC/CNTs substrate, the uniform coated high capacitance materials of Co3O4 nan...

متن کامل

The heterojunction effects of TiO2 nanotubes fabricated by atomic layer deposition on photocarrier transportation direction

The heterojunction effects of TiO2 nanotubes on photoconductive characteristics were investigated. For ITO/TiO2/Si diodes, the photocurrent is controlled either by the TiO2/Si heterojunction (p-n junction) or the ITO-TiO2 heterojunction (Schottky contact). In the short circuit (approximately 0 V) condition, the TiO2-Si heterojunction dominates the photocarrier transportation direction due to it...

متن کامل

Thermo-Optical Properties of Thin-Film TiO2–Al2O3 Bilayers Fabricated by Atomic Layer Deposition

We investigate the optical and thermo-optical properties of amorphous TiO2–Al2O3 thin-film bilayers fabricated by atomic layer deposition (ALD). Seven samples of TiO2–Al2O3 bilayers are fabricated by growing Al2O3 films of different thicknesses on the surface of TiO2 films of constant thickness (100 nm). Temperature-induced changes in the optical refractive indices of these thin-film bilayers a...

متن کامل

Photocatalytic Properties of Co3O4-Coated TiO2 Powders Prepared by Plasma-Enhanced Atomic Layer Deposition

Co3O4-coated commercial TiO2 powders (P25) p-n junction photocatalysts were prepared by plasma-enhanced atomic layer deposition (PEALD) technique. The structure, morphology, bandgap, and photocatalytic properties under ultraviolet light were investigated systematically. Although the deposition of Co3O4 does not change the anatase structure and crystallite size of P25 powders, the ultraviolet ph...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Nanoscale Research Letters

سال: 2019

ISSN: 1931-7573,1556-276X

DOI: 10.1186/s11671-019-2912-3