This study on surface-modifications of bulk oxidation catalysts with sub-monolayers PO x , BO and MnO via atomic layer deposition demonstrates this method to be a powerful tool for tuning the performance in selective oxidations light alkanes.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

ceramic surface modification of textiles by atomic layer deposition

24 Nanoscale ceramic surface modification of textiles by atomic layer deposition R ecent opportunities to merge traditional inorganic materials processing with organic fibrous textiles are creating new possibilities in electrical, optical and mechanical applications for textiles. Textiles are made of low-cost natural or synthetic fibers and have unique flexibility, strength and durability with ...

متن کامل

Atomic Layer Deposition of TiO

Additional resources and features associated with this article are available within the HTML version: • Supporting Information • Links to the 4 articles that cite this article, as of the time of this article download • Access to high resolution figures • Links to articles and content related to this article • Copyright permission to reproduce figures and/or text from this article High surface a...

متن کامل

Epitaxial graphene surface preparation for atomic layer deposition of Al2O3

Atomic layer deposition was employed to deposit relatively thick ( 30 nm) aluminum oxide (Al2O3) using trimethylaluminum and triply-distilled H2O precursors onto epitaxial graphene grown on the Si-face of silicon carbide. Ex situ surface conditioning by a simple wet chemistry treatment was used to render the otherwise chemically inert graphene surface more amenable to dielectric deposition. The...

متن کامل

Solar hydrogen generation by silicon nanowires modified with platinum nanoparticle catalysts by atomic layer deposition.

Covered with Pt: A uniform catalyst profile that ensures effective radial charge collection from high-aspect-ratio Si nanowires was achieved by atomic layer deposition of Pt nanoparticles. The resulting photoelectrode permits the measurement of high photovoltages and low overpotentials, and leads to very good stability against photooxidation of Si nanowires in solar water-reduction reactions.

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Catalysis Science & Technology

سال: 2023

ISSN: ['2044-4761', '2044-4753']

DOI: https://doi.org/10.1039/d2cy02184f