In the past 100 years, precipitation strengthening has always been extremely important pathway to resist deformation of material due significantly improving matrix strength. The size deviation degree and space distribution precipitates have a great influence on strength reported by recent experiments, however, this internal mechanism largely ignored incompletely understood until now in nickel-based superalloy. Herein, our work systematically clarifies effect complex interaction between dislocations 3D space, explore enrichment spatial mediated mechanism. Especially, new statistical approach using minimal spanning tree describe variation inter-precipitate spacing is proposed for accurately assessing contribution spatially randomly distributed Importantly, maximal occurs when variance equal average size, high frequent interactions with precipitations cause strong pinning distorted dislocation-line structure. slight precipitate corresponding optimal makes tend be evenly slip plane, which results more moving dislocation line, then leads severely curved dislocation, arising line tension inhibit its movement. A robustness test performed superalloys suggests method would robust evaluate performance without experiment, simultaneously gives distributions. current provides strategy adjust mode enhance mechanical properties hardened alloys.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Modelling of constitutive and fatigue behaviour of a single-crystal nickel-base superalloy

In this licentiate thesis the work done in the project KME410 will be presented. The overall objective of this project is to evaluate and develop tools for designing against fatigue in single-crystal nickel-base superalloys in gas turbines. Experiments have been done on single-crystal nickel-base superalloy specimens in order to investigate the mechanical behaviour of the material. The constitu...

متن کامل

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

High Temperature Deformation Mechanisms in a DLD Nickel Superalloy

The realisation of employing Additive Layer Manufacturing (ALM) technologies to produce components in the aerospace industry is significantly increasing. This can be attributed to their ability to offer the near-net shape fabrication of fully dense components with a high potential for geometrical optimisation, all of which contribute to subsequent reductions in material wastage and component we...

متن کامل

Joining of nickel-base superalloy single crystals

Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................

متن کامل

On APFIM of Grain Boundaries in a Nickel Base Superalloy

Experimental details of atom probe field ion microscopy (APFIM) of a Ni-16Cr-9Fe alloy are presented. In particular, studies concerning analysis of intergranular carbides and borides and segregation to grain boundaries are described. It was found that NiZ3B6 precipitates are very sensitive to preferential field evaporation, which necessitates optimization of the analysis conditions. In the FIM ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Plasticity

سال: 2022

ISSN: ['1879-2154', '0749-6419']

DOI: https://doi.org/10.1016/j.ijplas.2022.103333