Vanadia–titania multilayer nanodecoration of carbon onions via atomic layer deposition for high performance electrochemical energy storage
نویسندگان
چکیده
منابع مشابه
Ozone-Based Atomic Layer Deposition of Crystalline V2O5 Films for High Performance Electrochemical Energy Storage
A new atomic layer deposition (ALD) process for V2O5 using ozone (O3) as oxidant has been developed that resulted in crystalline V2O5 thin films which are single-phase and orthorhombic on various substrates (silicon, Au-coated stainless steel, and anodic aluminum oxide (AAO)) without any thermal post-treatment. Within a fairly narrow temperature window (170−185 °C), this low temperature process...
متن کاملRecent Development of Advanced Electrode Materials by Atomic Layer Deposition for Electrochemical Energy Storage
Electrode materials play a decisive role in almost all electrochemical energy storage devices, determining their overall performance. Proper selection, design and fabrication of electrode materials have thus been regarded as one of the most critical steps in achieving high electrochemical energy storage performance. As an advanced nanotechnology for thin films and surfaces with conformal interf...
متن کاملCarbon materials for the electrochemical storage of energy in capacitors
The electrochemical storage of energy in various carbon materials (activated carbons, aerogels, xerogels, nanostructures) used as capacitor electrodes is considered. Different types of capacitors with a pure electrostatic attraction and/or pseudocapacitance effects are presented. Their performance in various electrolytes is studied taking into account the different range of operating voltage (1...
متن کاملAtomic layer deposition encapsulated activated carbon electrodes for high voltage stable supercapacitors.
Operating voltage enhancement is an effective route for high energy density supercapacitors. Unfortunately, widely used activated carbon electrode generally suffers from poor electrochemical stability over 2.5 V. Here we present atomic layer deposition (ALD) encapsulation of activated carbons for high voltage stable supercapacitors. Two-nanometer-thick Al2O3 dielectric layers are conformally co...
متن کاملCNFs @ CNTs : Superior Carbon for Electrochemical Energy Storage * *
** The authors are indebted to the Max Planck Society and acknowledge support within the framework of the ENERCHEM project. The authors would like to acknowledge technical assistance from the Combicat Centre, Universiti Malaya (Kuala Lumpur, Malaysia); Edith Kitzelmann, Fritz-Haber-Institut; and Dr. Andreja Gajović, Molecular Physics Laboratory, Rudjer Boskovic Institute (Zagred, Croatia). Supp...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Materials Chemistry A
سال: 2017
ISSN: 2050-7488,2050-7496
DOI: 10.1039/c6ta09890h