Weld crack susceptibility of duplex stainless steel. (Report V). Numerical analysis on solidification brittleness temperature range in stainless steel.

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Crystallography of Widmanstätten austenite in duplex stainless steel weld metal

Two kinds of austenite grow from d-ferrite during the cooling of the duplex stainless steel weld deposits studied here, Widmanstätten plates and allotriomorphs which precipitate at d–d grain boundaries. It is found using microtexture measurements that the preferred crystallographic orientation of the Widmanstätten austenite can be estimated using established theory if it is assumed that there i...

متن کامل

Study on Static Recrystallization Process in Duplex Stainless Steel 2205

Steel 2205 is one of the most famous duplex stainless steels. The microstructure of this steel composed of ferrite and austenite in similar amount. Therefore, in order to improve mechanical properties through microstructure, thermo mechanical processes such as controlled hot rolling and forging should be applied. It is not possible to employ the usual heat treatment. It shows the importance of ...

متن کامل

Stainless steel weld metal designed to mitigate residual stresses

There have been considerable efforts to create welding consumables which on solid state phase transformation partly compensate for the stresses which develop when a constrained weld cools to ambient temperatures. All of these efforts have focused on structural steels which are ferritic. In the present work, alloy design methods have been used to create a stainless steel welding consumable which...

متن کامل

Stress Corrosion Crack Growth Mechanism on SUS316L Stainless Steel

The stress corrosion cracking (SCC) of stainless steel is one of the biggest problems for maintaining atomic power and chemical plants. However the mechanism has not been solved because of difficulty in observing hydrogen movement. In order to solve this problem, the author has developed a new SCC test method that enables the super Kelvin force microscope (SKFM) and the Kelvin force microscope ...

متن کامل

Kinetics of Sigma Phase Formation In a Duplex Stainless Steel

This work determines the kinetics of sigma phase formation in UNS S31803 Duplex Stainless Steel (DSS), describing the phase transformations that occur in isothermal aging between 700 and 900 °C for time periods up to 1032 hours, allowing the determination of the Time-Temperature-Precipitation (TTP) diagram for sigma phase and proposing a model to predict the kinetics of sigma phase formation us...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY

سال: 1991

ISSN: 0288-4771

DOI: 10.2207/qjjws.9.93