Welding procedure qualification record (WPQR) for welds fabricated at proximity
نویسندگان
چکیده
Abstract Maintaining the minimum allowable distance between proximity welds has always been considered a subject of debate among design engineers, welding engineers/inspectors and fabricators/engineering contractors. The scattered nature guidelines available in codes standards for maintaining poses significant challenge procedure inspection criteria development process. This is especially critical complex welded joints on submerged sections offshore structures, compact layouts/branched connections topside piping components, structural (depending complexity). manuscript presents findings an experimental study that was performed by fabricating two girth at S355 steel tubular section with diameter 219.1 mm thickness 8.18 mm. Proximity were fabricated three different distances their weld toes, 5, 10, 15 mm, respectively, using procedures. Welding qualification record (WPQR) performed, all prescribed mechanical tests recorded as per NORSOK M-101, fabrication code. Although results from test met specified values defined code, research revealed noticeable difference Charpy hardness region adjacent welds. Considerable changes final microstructure morphology observed due to varying thermal cycles. These observations can form basis future joints, structures during replacement/repair procedures layouts.
منابع مشابه
Qualification of a Robotic Pipeline Orbital Welding
This work presents the procedure qualification for pipeline orbital welding using a robotic system. The system has four degrees of freedom, which allow the controlling of the stick out, the travel speed, the torch angle and the positioning. The arc voltage and welding current are also controlled during the welding, although the system uses a conventional power source. With the system it is poss...
متن کاملMicrostructure, Welding Mechanism, and Failure of Al/Cu Ultrasonic Welds
Ultrasonic metal welding has been used widely to join battery cell terminals, or tabs (either Al or Cu), with bus bars (Cu) to form assembled battery packs in battery electric vehicles. However, the mechanism of ultrasonic welding for Al/Cu is still not well understood. In this work, the microstructures of the ultrasonic welds between three layers of lithium-ion battery tabs (either Al or Cu) a...
متن کاملA declarative semantics for CLP with qualification and proximity
Uncertainty in Logic Programming has been investigated during the last decades, dealing with various extensions of the classical LP paradigm and different applications. Existing proposals rely on different approaches, such as clause annotations based on uncertain truth values, qualification values as a generalization of uncertain truth values, and unification based on proximity relations. On th...
متن کاملA Transformation-based implementation for CLP with qualification and proximity
To appear in Theory and Practice of Logic Programming (TPLP) Uncertainty in logic programming has been widely investigated in the last decades, leading to multiple extensions of the classical LP paradigm. However, few of these are designed as extensions of the well-established and powerful CLP scheme for Constraint Logic Programming. In a previous work we have proposed the SQCLP (proximity-base...
متن کاملFixpoint & Proof-theoretic Semantics for CLP with Qualification and Proximity
Uncertainty in Logic Programming has been investigated during the last decades, dealing with various extensions of the classical LP paradigm and different applications. Existing proposals rely on different approaches, such as clause annotations based on uncertain truth values, qualification values as a generalization of uncertain truth values, and unification based on proximity relations. On th...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: The International Journal of Advanced Manufacturing Technology
سال: 2022
ISSN: ['1433-3015', '0268-3768']
DOI: https://doi.org/10.1007/s00170-022-09022-5