X-ray diffraction study on inelastic deformation behavior of Ni-base single crystal superalloy

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

X-ray Stress Measurement of Nickel-base Single Crystal Superalloy Using Two-dimensional Detector

The stress in a single crystal of nickel-base superalloy with 72 % volume fraction of '-phase was measured by the X-ray method. The specimen whose surface normal was parallel to [001] direction was oscillated around -axis during recording of the X-ray diffraction pattern with a two-dimensional position sensitive proportional counter (PSPC). The stress was determined from the measured strain u...

متن کامل

Fretting on the cubic face of a single-crystal Ni-base superalloy at room temperature

Fretting experiments were conducted on the (10 0) crystal (cubic) face of a single crystal Ni-base superalloy in two directions, /10 0S and /110S, to study the effect of crystallographic orientation on the fretting response in both partial slip and gross slip regimes. The study involved point contacts using a tungsten carbide (WC) ball with radius 10 mm tested at room temperature. Ball indentat...

متن کامل

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

Deformation compatibility in a single crystalline Ni superalloy

Deformation in materials is often complex and requires rigorous understanding to predict engineering component lifetime. Experimental understanding of deformation requires utilization of advanced characterization techniques, such as high spatial resolution digital image correlation (HR-DIC) and high angular resolution electron backscatter diffraction (HR-EBSD), combined with clear interpretatio...

متن کامل

Crystal structure of Ni-sorbed synthetic vernadite: A powder X-ray diffraction study

15 16 Vernadite is a nanocrystalline turbostratic phyllomanganate ubiquitous in the environment, 17 which contains nickel in specific settings such as oceanic sediments. To improve our 18 understanding of nickel uptake in this mineral, two series of synthetic analogs to vernadite (δ19 MnO2) were prepared with Ni/Mn atomic ratios ranging from 0.002 to 0.105 at pH 4 and from 20 0.002 to 0.177 at ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia Structural Integrity

سال: 2016

ISSN: 2452-3216

DOI: 10.1016/j.prostr.2016.06.115