XPS, SEM, DSC and Nanoindentation Characterization of Silver Nanoparticle-Coated Biopolymer Pellets

نویسندگان

چکیده

The development of environmentally friendly materials has been the focus many research groups in recent years due to increased harmful effects plastics on environment. Bio-based are considered a key solution from sustainable manufacturing perspective. nano-coating biopolymer blends with silver nanoparticles is subject challenging projects line EU Directive environment protection and manufacturing. Coating biopolymers provides an antimicrobial antiviral active surface. In this work, we develop nanoparticle-coated Arboblend V2 Nature pellets. main goal obtain new material antibacterial action obtained blending pellets through physical vapor deposition. study divided three steps. first step represents characterization coated/raw second involves injection molding nano-coated samples obtained. last regards press coated order thin films, as well their characterization. PVD-sputtering technique used coat nanoparticles. This process especially optimized for coating raw high water content small-size mechanical properties, surface chemical composition thermal properties both virgin measured analyzed resistance layer. Differential scanning calorimetry, electron microscopy, X-ray photoemission spectroscopy nanoindentation testing performed. calorimetry test detects no significant alteration produced PVD confirms viable application nano-silver–biopolymer composite products.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Characterization of tungsten tips for STM by SEM/AES/XPS

For the first time, both X-ray Photoelectron Spectroscopy (XPS) and Auger Electron Spectroscopy (AES) techniques were applied in analysis of surface contamination of electrochemically etched Scanning Tunneling Microscope (STM) tungsten tips. Carbon monoxide, graphite, tungsten carbide and tungsten oxide were found as main surface contaminations of STM tungsten tips. The thickness of tungsten ox...

متن کامل

extraction and characterization of allium irancum plant extract and its application in the green synthesis of silver nano particles and oxidation of thiocarbony1 compounds

سنتز سبز نانوذرات فلزی (nps) درسالهای اخیر توجه بسیارزیادی را به خود جلب کرده است. زیرا این پروتوکل کم هزینه وسازگار با محیط زیست از روش های استاندارد سنتز. در این پایان نامه ما گزارش میکنیم یک روش ساده و سازگار با محیط زیست برای سنتز نانوذرات نقره با استفاده از محلول آبی عصاره گیاه allium iranicum به عنوان یک عامل کاهش دهنده ی طبیعی. نانو ذرات نقره مشخص شد با استفاده از تکنیک های uv-visible، x...

Antimicrobial characterization of silver nanoparticle-coated surfaces by “touch test” method

Bacterial infections, especially by antimicrobial resistant (AMR) bacteria, are an increasing problem worldwide. AMR is especially a problem with health care-associated infections due to bacteria in hospital environments being easily transferred from patient to patient and from patient to environment, and thus, solutions to prevent bacterial transmission are needed. Hand washing is an effective...

متن کامل

Dataset on the physical characterization of biopolymer coated magnetic nanoparticles

The data presented in this article is related to the research article entitled "Paclitaxel loaded magnetic nanocomposites with folate modified chitosan/carboxymethyl surface; a vehicle for imaging and targeted drug delivery" (S. Bano, M. Afzal, M.M. Waraich, K. Alamgir, S. Nazir, 2016) [1]. It contains the absorbance spectra, band gap energies of pure nickel-ferrite nano cores (NFs), and calibr...

متن کامل

Biosynthesis of Silver nanoparticle using aqueous extract of Saraca asoca leaves, its characterization and antimicrobial activity

The use of less hazardous chemicals or natural material in place of toxic chemical for the formation of metal nanoparticle is known as green synthesis. The present paper deals with greener approach for the synthesis of silver (Ag) nanoparticles. The Saraca asoca plant leaves extract solution was used for the silver nanoparticles. Confirmation of Ag nanoparticles has been done using var...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied sciences

سال: 2021

ISSN: ['2076-3417']

DOI: https://doi.org/10.3390/app11167706