effect of mechanical load cycling on microtensile bond strength of self-etch systems to dentin

نویسندگان

sh. kasraei associate professor, department of operative dentistry, school of dentistry, hamadan university of m

z. khamverdi 2associate professor, dental research center, hamadan university of medical sciences, hamadan, iran

چکیده

objective: optimal dentin bonding is not always obtained in clinical practice due to func-tional forces. these forces may provide stresses throughout the tooth and restorative sys-tem, which in turn may affect the adhesive bond. this experimental study evaluated the effect of load cycling on bond strength of self-etch systems. materials and methods: one third of the coronal portions of 48 intact human extractedupper premolars were removed. the teeth were equally divided into six groups. in groups unloaded-clear tri-s bond (ulcb) and loaded-clear tri-s bond (lcb), prepared dentin surfaces of each tooth were treated with clearfil tri-s bond (kurary medical inc, oka-yama, japan), in groups unloaded-i bond (ulib) and loaded-i bond (lib) with i bond heraeus kulzer, gmbh,&co; kg, germany), and in groups unloaded-xeno iii (ulx) and loaded-xeno iii (lx) with xeno iii dentin adhesives (dentsply detrey gmbh, kon-stanz, germany). then, the teeth were restored with filtek supreme resin composite. after thermal cycling of the samples, groups lcb, lib and lx were submitted to mechanical loading (100,000 cycles, 60 n). microtensile bond strength (mtbs) test was performed for all of groups. two-way anova and tukey hsd tests served for statistical analysis. results: results showed that groups ulcb and ulib had significantly more bond strength than group ulx (p<0.05). for all the tree adhesive systems, the mtbs values in teeth subjected to load cycling was significantly lower than unloaded teeth (p<0.001). conclusion: load cycling seems to decrease mtbss of one-step adhesive systems to den-tin.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of long-term water aging on microtensile bond strength of self-etch adhesives to dentin.

PURPOSE To evaluate the effect of water storage on the microtensile dentin bond strength of one total-etch and four self-etching adhesives to dentin. METHODS The adhesive materials were: one total-etch adhesive (Admira Bond) and four self-etch adhesives (Clearfil S tri Bond, Hybrid Bond, Futurabond NR, Adhe SE). Freshly extracted human third molar teeth were used. For each tooth, dentin was e...

متن کامل

Effects of blood contamination on microtensile bond strength to dentin of three self-etch adhesives.

This study evaluated the effects of blood contamination and decontamination methods during different steps of bonding procedures on the microtensile bond strength of two-step self-etch adhesives to dentin. Sixty extracted human molars were ground flat to expose occlusal dentin. The 60 molars were randomly assigned to three groups, each treated with a different two-step self-etch adhesive: Clear...

متن کامل

Effects of Thermal and Mechanical Load Cycling on the Dentin Microtensile Bond Strength of Single Bond-2

BACKGROUND Different studies have shown the uncertain effects of thermal cycling (TC) and mechanical load cycling (MC) on the dentin microtensile bond strength (µTBS) of composites. This study designed to investigate the effects of TC and MC on the dentin µTBS of single bond-2. MATERIALS AND METHODS Flat dentinal surface was prepared on 48 sound extracted human third molar teeth, and were bon...

متن کامل

Effect of Airborne Particle Abrasion on Microtensile Bond Strength of Total-Etch Adhesives to Human Dentin

Aim of this study was to investigate a specific airborne particle abrasion pretreatment on dentin and its effects on microtensile bond strengths of four commercial total-etch adhesives. Midcoronal occlusal dentin of extracted human molars was used. Teeth were randomly assigned to 4 groups according to the adhesive system used: OptiBond FL (FL), OptiBond Solo Plus (SO), Prime & Bond (PB), and Ri...

متن کامل

Microtensile bond strength of clearfil SE bond to caries-affected dentin and normal dentin

Microtensile bond strength of clearfil SE bond to caries-affected dentin and normal dentin Dr. A. Ghasemi* - Dr. M. Bargrizan** - Dr. M. Mahmoodi*** *- Assistant Professor of Operative Dentistry Dept. - Faculty of Dentistry – Shaheed Beheshti University of Medical Sciences. **- Assistant Professor of Pedodontics Dept. - Faculty of Dentistry – Shaheed Beheshti University of Medical Sciences. ***...

متن کامل

Sodium fluoride addition to a two-step etch-and-rinse adhesive system: effect on dentin microtensile bond strength and durability

Introduction: Studies have suggested that sodium fluoride (NaF) has an inhibitory effect on the activity of endogenous matrix metalloproteinase enzymes. This study assessed the effect of a fluoride-containing adhesive on microtensile bond&nbsp;strength (&micro;TBS) over time. Material & Methods: In this experimental study, 36 extracted &nbsp;third molars were used to evaluate the &micro;TBS of...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید


عنوان ژورنال:
journal of dentistry, tehran university of medical sciences

جلد ۵، شماره ۴، صفحات ۱۷۳-۱۷۸

کلمات کلیدی

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023